Ductile Iron in ASTM A536
Ductile iron grades in ASTM A536: Gr 60-40-18, Gr 65-45-12, Gr 80-55-06, Gr 100-70-03, Gr 120-90-02,Gr 60-42-10,Gr 70-50-05,Gr 80-60-03
Casting Technology, include casting methods, casting material and casting standards.
Ductile iron grades in ASTM A536: Gr 60-40-18, Gr 65-45-12, Gr 80-55-06, Gr 100-70-03, Gr 120-90-02,Gr 60-42-10,Gr 70-50-05,Gr 80-60-03
GGG40, GGG50, GGG60, GGG70, GGG80, GGG-35.3,GGG-40.3 in Din 1693
Grade 80-40 [550-275] UNSD50400 in ASTM A148 for Sand Casting and Investment Casting
Stainless steel CA6NM (UNS J91540) in ASTM A743 and ASTM A352 and ASTM 487; E3N in ASTM A757 casting standard
Carbon Manganese steel LCC (UNS J02505) in ASTM A352 casting standard
Stainless Steel CC50 (UNS J92615) in ASTM A743 Casting Standard
Stainless Steel CB30 (UNS J91803) in ASTM A743 Casting Standard
Stainless Steel CA15M (UNS J91151) in ASTM A743 and ASTM A487 Casting Standard
Stainless Steel CE30 (UNS J93423) in ASTM A743 casting standard
Stainless Steel CF16F (UNS J92701) in ASTM A743 standard