GGG-50 (EN 0.7050) Ductile Cast Iron Casting Material
Ductile Cast Iron
Introduction
DIN 1693-1 and DIN 1693-2 Grade GGG-50 is a ductile cast iron grade. Process options include sand casting, shell molding and lost-foam casting. Typical family applications include gear and transmission components, hubs, brackets, machine housings and pump-related castings.
| Field | Value |
|---|---|
| Designation | GGG-50 (EN 0.7050) |
| Material Type | Cast Iron |
| Sub Type | Ductile Cast Iron |
| Product Form | casting |
Manufacturing Process
Sand Casting
Shell Molding Casting
Lost Foam Casting
Equivalent Materials
| Standard | Material Grade |
|---|---|
| NBN 830-02 | FNG50-7 |
| NS11 301 | SJK-500 |
| NF A32-201 | FGS500-7 |
| EN 1563 | EN-GJS-500-7 |
| JIS G5502 | FCD500 |
| UNI 4544 | GS500-7 |
| AS 1831 | 500-7 |
| SAE J434 | D500 |
| SS 14 07 | 0727-02 |
| BS 2789 | 500/7 |
| IS 1865 | SG500/7 |
| UNE 36-118 | FGE50-7 |
| ASTM A536 | 70-50-05 |
| GB/T 1348 | QT500-7 |
| ISO 1083 | ISO1083/JS/500-7 |
Approximate materials; not guaranteed interchangeable.
Similar Materials
Not Available
Reference Standards
| Standard | Standard Title | Edition | Specification | Identifier |
|---|---|---|---|---|
| DIN 1693-1 | Cast Iron with Nodular Graphite — Unalloyed and Low Alloy Grades | 1973-10 | GGG-50 | DIN 0.7050 |
| DIN 1693-2 | Cast Iron with Nodular Graphite — Unalloyed and Low Alloy Grades — Properties in Cast-on Test Piece | 1977-10 | GGG-50 | DIN 0.7050 |
Related Casting Products
Physical Properties
| Property | Value | Applicable Conditions |
|---|---|---|
| Density | 7.2 kg/dm³ |
- Sources: DIN 1693-1:1973-10
- Approximate density for weight calculations, not a guaranteed density limit.
- Informative values; not mandatory acceptance limits.
Chemical Composition
DIN 1693-1–1973-10
No specified chemical composition limits in DIN 1693-1
DIN 1693-2–1977-10
Not Available
Heat Treatment
Separately cast test piece — Supplied as cast or heat-treated; no mandatory numerical heat-treatment cycle specified.
Sources: DIN 1693-1:1973-10
DIN 1693-2–1977-10
Not Available
Mechanical Properties
Primary Mechanical Properties
DIN 1693-1 — 1973-10
Condition: Separately cast test piece
| Property | Requirement |
|---|---|
| Tensile Strength | ≥ 500 N/mm² |
| Yield Strength (Rp0.2) | ≥ 320 N/mm² |
| Elongation | ≥ 7 % |
- Specimen dimensions and number are agreed; otherwise manufacturer decides. Test-piece thickness should approximate ruling casting thickness. For sections >50 mm and compact castings, agreement is urged; these are separately cast test-piece guarantees, not universal casting-location minima.
- Separately cast U or Y test piece
- tensile specimen per DIN 50125
- A5 elongation
DIN 1693-2 — 1977-10
Condition: Cast-on test piece 40 mm; DIN 50125 B14x70 tensile specimen; A5 elongation; 30 ≤ t ≤ 60 mm; Cast-on test piece
| Property | Requirement |
|---|---|
| Tensile Strength | ≥ 450 N/mm² |
| Yield Strength (Rp0.2) | ≥ 300 N/mm² |
| Elongation | ≥ 7 % |
- Cast-on test pieces remain attached until heat treatment is complete, except stress relief that does not modify structure. Side-cast specimens are taken from the bottom two-thirds.
- Primarily casting weights >2000 kg and/or sections 50–200 mm
- other sizes need separate agreement. Table 1 specifically lists 30–60 and >60–200 mm.
DIN 1693-2 — 1977-10
Condition: Cast-on test piece 70 mm; DIN 50125 B14x70 tensile specimen; A5 elongation; 60 < t ≤ 200 mm; Cast-on test piece
| Property | Requirement |
|---|---|
| Tensile Strength | ≥ 420 N/mm² |
| Yield Strength (Rp0.2) | ≥ 290 N/mm² |
| Elongation | ≥ 5 % |
- Cast-on test pieces remain attached until heat treatment is complete, except stress relief that does not modify structure. Side-cast specimens are taken from the bottom two-thirds.
- Primarily casting weights >2000 kg and/or sections 50–200 mm
- other sizes need separate agreement. Table 1 specifically lists 30–60 and >60–200 mm.
DIN 1693-2 — 1977-10
Condition: Informative casting-location design guidance
Informative
| Property | t ≤ 50 mm | 50 < t ≤ 80 mm | 80 < t ≤ 120 mm | 120 < t ≤ 200 mm |
|---|---|---|---|---|
| Yield Strength (Rp0.2) | ≥ 290 N/mm² | ≥ 280 N/mm² | ≥ 270 N/mm² | ≥ 260 N/mm² |
- Casting location, not separately cast or cast-on specimen
- Guidance for design only
- not guaranteed casting minima. At junctions use largest inscribable cylinder diameter rather than nominal wall thickness
- approximately 95% probability of being exceeded.
- Informative reference value
- not an acceptance requirement
Welding Conditions
Not Available
Applications
Typical cast components in this material family include gear and transmission components, hubs, brackets, machine housings and pump-related castings. Applications include agricultural, construction and general industrial machinery. Lifting, low-temperature and pressure-retaining duties require the relevant component-specific requirements; ordinary family uses do not establish those capabilities.