Class 400 Grey Cast Iron Casting Material

Grey Cast Iron

Download MDS PDF · Request a Quote

Introduction

ASTM A48/A48M Class 400 is a gray iron casting grade. The metric series uses separately cast tensile bars to establish the class minimum. The specification covers general engineering castings where tensile strength is a major consideration.

FieldValue
DesignationClass 400
Material TypeCast Iron
Sub TypeGrey Cast Iron
Product Formcasting

Manufacturing Process

Sand Casting
Shell Molding Casting
Lost Foam Casting

Equivalent Materials

Not Available

Similar Materials

Not Available

Reference Standards

StandardStandard TitleEditionSpecification
ASTM A48/A48MStandard Specification for Gray Iron Castings03Class 400

Physical Properties

Not Available

Chemical Composition

No specified chemical composition limits in ASTM A48/A48M

Heat Treatment

ASTM A48/A48M–03

No heat treatment specified in ASTM A48/A48M

Mechanical Properties

Primary Mechanical Properties

ASTM A48/A48M — 03

Condition: Separately cast test bars (Metric)

PropertyRequirement
Tensile Strength≥ 400 MPa[1][2][3][4][5][6][7][8][9][10][11][12][13]

Notes

  • [1] Class 400A: Test bar diameter: 20–22 mm; applicable casting wall thickness: 5–14 mm if no specific bar-to-casting correlation is established. As-cast bar: 22.4 mm nominal mid-length diameter, 21.6 mm minimum bottom diameter, 24.4 mm maximum top diameter; minimum length 125 mm (recommended maximum 150 mm). Specimen A, machined concentric with the test-bar axis. Minimum time from loading to fracture: 15 s.
  • [2] Class 400B: Test bar diameter: 30 mm; applicable casting wall thickness: 15–25 mm if no specific bar-to-casting correlation is established. As-cast bar: 30.5 mm nominal mid-length diameter, 29.0 mm minimum bottom diameter, 33.5 mm maximum top diameter; minimum length 150 mm (recommended maximum 230 mm). Specimen B, machined concentric with the test-bar axis. Minimum time from loading to fracture: 20 s.
  • [3] Class 400C: Test bar diameter: 50 mm; applicable casting wall thickness: 26–50 mm if no specific bar-to-casting correlation is established. As-cast bar: 50.8 mm nominal mid-length diameter, 48.3 mm minimum bottom diameter, 53.3 mm maximum top diameter; minimum length 175 mm (recommended maximum 255 mm). Specimen B or C, machined concentric with the test-bar axis. The manufacturer selects the type unless the purchaser specifies it in writing. Minimum time from loading to fracture: 20 s.
  • [4] Class 400S: Applicable casting wall thickness: under 5 mm or over 50 mm if no specific bar-to-casting correlation is established. The manufacturer and purchaser agree on all test bar dimensions and on the nature and dimensions of the tensile specimen. No separate loading-to-fracture minimum is specified for S.
  • [5] The minimum applies to separately cast test coupons. Tensile strength can vary across the section of a casting.
  • [6] Apply the inch-pound and SI values independently. They are not exact equivalents.
  • [7] Cast test bars separately from the same lot. Use dried, baked or chemically bonded silica-sand molds with suitable binders and similar sand grain size to the casting molds. The molds must be approximately at room temperature when poured, with surrounding sand at least one bar diameter thick.
  • [8] When the casting is cooled in the mold below 480 °C before shakeout, cool the test bar in its mold below 480 °C before optional still-air cooling to room temperature. For castings shaken out above 480 °C, either follow that route or, by manufacturer–purchaser agreement, shake out the bar at about the casting temperature.
  • [9] If insufficient separately cast test pieces are available, a specimen may be taken from a representative location on a casting by manufacturer–purchaser agreement.
  • [10] Informative: If a casting-to-coupon correlation is needed, testing may establish it. If reliable correlation data are unavailable and testing is impracticable, select a test casting approximating the main or controlling casting section.
  • [11] Apply the tensile load axially. The standard cites ASTM E 8 for the test method.
  • [12] If a casting is stress-relieved, annealed, or otherwise heat-treated, give its representative test bars the same treatment alongside the castings.
  • [13] If the first test shows that heat treatment is needed to meet the requirements, treat the entire casting lot and its representative test specimens together, then perform the required testing. After a valid nonconforming test, make two retests and reject the represented castings if either retest fails.

Welding Conditions

ASTM A48/A48M — 03

PropertyValue
Post-weld Heat TreatmentInformative: Where practical, suitable post-weld heat treatment may reduce adverse effects of welding on the casting.[1][2]

Notes

  • [1] Informative option after authorized welding repair; The standard prohibits repair by plugging or welding unless the purchaser gives written permission.
  • [2] Informative values; not mandatory acceptance limits.

Applications

Gray iron ASTM A48M Class 400 belongs to the gray iron family used for machinery castings. Machine-tool heads and pump or compressor components illustrate common family uses. The required grade for each casting depends on the part design and acceptance requirements.

Need Class 400 Castings?

Contact us for casting and machining inquiries.

Last Updated: November 25, 2026

error: Alert: Thanks for your interesting, but Article is protected ! You can click the Top Right email!