Class 350 Grey Cast Iron Casting Material

Grey Cast Iron

Download MDS PDF · Request a Quote

Introduction

ASTM A48/A48M Class 350 is a gray iron casting grade. To qualify the metric class, the specification applies its strength minimum to a separately cast bar. The specification covers general engineering castings where tensile strength is a major consideration.

FieldValue
DesignationClass 350
Material TypeCast Iron
Sub TypeGrey Cast Iron
Product Formcasting

Manufacturing Process

Sand Casting
Shell Molding Casting
Lost Foam Casting

Equivalent Materials

StandardMaterial Grade
SAE J431G13H24
DIN 1691GG35
NS11 100SJG350
GB/T 9439HT350
UNI 5007G35
SS 14 01O135
UNFFG35
BS 1452350
JIS G5501FC350
AS 1830350
IS 210FG350
EN 1561EN-GJL-350
NG A32-101FGL350
NBN 830-01FGG35
ISO 185ISO 185/JL/350

Approximate materials; not guaranteed interchangeable.

Similar Materials

Not Available

Reference Standards

StandardStandard TitleEditionSpecification
ASTM A48/A48MStandard Specification for Gray Iron Castings03Class 350

Physical Properties

Not Available

Chemical Composition

No specified chemical composition limits in ASTM A48/A48M

Heat Treatment

ASTM A48/A48M–03

No heat treatment specified in ASTM A48/A48M

Mechanical Properties

Primary Mechanical Properties

ASTM A48/A48M — 03

Condition: Separately cast test bars (Metric)

PropertyRequirement
Tensile Strength≥ 350 MPa[1][2][3][4][5][6][7][8][9][10][11][12][13]

Notes

  • [1] Class 350A: Test bar diameter: 20–22 mm; applicable casting wall thickness: 5–14 mm if no specific bar-to-casting correlation is established. As-cast bar: 22.4 mm nominal mid-length diameter, 21.6 mm minimum bottom diameter, 24.4 mm maximum top diameter; minimum length 125 mm (recommended maximum 150 mm). Specimen A, machined concentric with the test-bar axis. Minimum time from loading to fracture: 15 s.
  • [2] Class 350B: Test bar diameter: 30 mm; applicable casting wall thickness: 15–25 mm if no specific bar-to-casting correlation is established. As-cast bar: 30.5 mm nominal mid-length diameter, 29.0 mm minimum bottom diameter, 33.5 mm maximum top diameter; minimum length 150 mm (recommended maximum 230 mm). Specimen B, machined concentric with the test-bar axis. Minimum time from loading to fracture: 20 s.
  • [3] Class 350C: Test bar diameter: 50 mm; applicable casting wall thickness: 26–50 mm if no specific bar-to-casting correlation is established. As-cast bar: 50.8 mm nominal mid-length diameter, 48.3 mm minimum bottom diameter, 53.3 mm maximum top diameter; minimum length 175 mm (recommended maximum 255 mm). Specimen B or C, machined concentric with the test-bar axis. The manufacturer selects the type unless the purchaser specifies it in writing. Minimum time from loading to fracture: 20 s.
  • [4] Class 350S: Applicable casting wall thickness: under 5 mm or over 50 mm if no specific bar-to-casting correlation is established. The manufacturer and purchaser agree on all test bar dimensions and on the nature and dimensions of the tensile specimen. No separate loading-to-fracture minimum is specified for S.
  • [5] The minimum applies to separately cast test coupons. Tensile strength can vary across the section of a casting.
  • [6] Apply the inch-pound and SI values independently. They are not exact equivalents.
  • [7] Cast test bars separately from the same lot. Use dried, baked or chemically bonded silica-sand molds with suitable binders and similar sand grain size to the casting molds. The molds must be approximately at room temperature when poured, with surrounding sand at least one bar diameter thick.
  • [8] When the casting is cooled in the mold below 480 °C before shakeout, cool the test bar in its mold below 480 °C before optional still-air cooling to room temperature. For castings shaken out above 480 °C, either follow that route or, by manufacturer–purchaser agreement, shake out the bar at about the casting temperature.
  • [9] If insufficient separately cast test pieces are available, a specimen may be taken from a representative location on a casting by manufacturer–purchaser agreement.
  • [10] Informative: If a casting-to-coupon correlation is needed, testing may establish it. If reliable correlation data are unavailable and testing is impracticable, select a test casting approximating the main or controlling casting section.
  • [11] Apply the tensile load axially. The standard cites ASTM E 8 for the test method.
  • [12] If a casting is stress-relieved, annealed, or otherwise heat-treated, give its representative test bars the same treatment alongside the castings.
  • [13] If the first test shows that heat treatment is needed to meet the requirements, treat the entire casting lot and its representative test specimens together, then perform the required testing. After a valid nonconforming test, make two retests and reject the represented castings if either retest fails.

Welding Conditions

ASTM A48/A48M — 03

PropertyValue
Post-weld Heat TreatmentInformative: Where practical, suitable post-weld heat treatment may reduce adverse effects of welding on the casting.[1][2]

Notes

  • [1] Informative option after authorized welding repair; The standard prohibits repair by plugging or welding unless the purchaser gives written permission.
  • [2] Informative values; not mandatory acceptance limits.

Applications

Gray iron ASTM A48M Class 350 belongs to a casting family with applications in machinery and fluid handling. Gray iron examples include machine-tool heads and components for pumps and compressors. The equipment design and acceptance requirements guide the grade selection.