Introduction
ASTM A48/A48M Class 150 is a gray iron casting grade. Its metric classification uses the minimum tensile strength of separately cast test bars. The specification covers general engineering castings where tensile strength is a major consideration.
| Field | Value |
|---|---|
| Designation | Class 150 |
| Material Type | Cast Iron |
| Sub Type | Grey Cast Iron |
| Product Form | casting |
Manufacturing Process
Sand Casting
Shell Molding Casting
Lost Foam Casting
Equivalent Materials
| Standard | Material Grade |
|---|---|
| AS 1830 | 150 |
| BS 1452 | 150 |
| DIN 1691 | GG15 |
| SS 14 01 | O115 |
| SAE J431 | G9H12 |
| GB/T 9439 | HT150 |
| NBN 830-01 | FGG15 |
| UNI 5007 | G15 |
| UNF | FG15 |
| NG A32-101 | FGL150 |
| NS11 100 | SJG150 |
| JIS G5501 | FC150 |
| IS 210 | FG150 |
| EN 1561 | EN-GJL-150 |
| ISO 185 | ISO 185/JL/150 |
Approximate materials; not guaranteed interchangeable.
Similar Materials
Not Available
Reference Standards
| Standard | Standard Title | Edition | Specification |
|---|---|---|---|
| ASTM A48/A48M | Standard Specification for Gray Iron Castings | 03 | Class 150 |
Related Casting Products
Physical Properties
Not Available
Chemical Composition
No specified chemical composition limits in ASTM A48/A48M
Heat Treatment
ASTM A48/A48M–03
No heat treatment specified in ASTM A48/A48M
Mechanical Properties
Primary Mechanical Properties
ASTM A48/A48M — 03
Condition: Separately cast test bars (Metric)
Notes
- [1] Class 150A: Test bar diameter: 20–22 mm; applicable casting wall thickness: 5–14 mm if no specific bar-to-casting correlation is established. As-cast bar: 22.4 mm nominal mid-length diameter, 21.6 mm minimum bottom diameter, 24.4 mm maximum top diameter; minimum length 125 mm (recommended maximum 150 mm). Specimen A, machined concentric with the test-bar axis. Minimum time from loading to fracture: 15 s.
- [2] Class 150B: Test bar diameter: 30 mm; applicable casting wall thickness: 15–25 mm if no specific bar-to-casting correlation is established. As-cast bar: 30.5 mm nominal mid-length diameter, 29.0 mm minimum bottom diameter, 33.5 mm maximum top diameter; minimum length 150 mm (recommended maximum 230 mm). Specimen B, machined concentric with the test-bar axis. Minimum time from loading to fracture: 20 s.
- [3] Class 150C: Test bar diameter: 50 mm; applicable casting wall thickness: 26–50 mm if no specific bar-to-casting correlation is established. As-cast bar: 50.8 mm nominal mid-length diameter, 48.3 mm minimum bottom diameter, 53.3 mm maximum top diameter; minimum length 175 mm (recommended maximum 255 mm). Specimen B or C, machined concentric with the test-bar axis. The manufacturer selects the type unless the purchaser specifies it in writing. Minimum time from loading to fracture: 20 s.
- [4] Class 150S: Applicable casting wall thickness: under 5 mm or over 50 mm if no specific bar-to-casting correlation is established. The manufacturer and purchaser agree on all test bar dimensions and on the nature and dimensions of the tensile specimen. No separate loading-to-fracture minimum is specified for S.
- [5] The minimum applies to separately cast test coupons. Tensile strength can vary across the section of a casting.
- [6] Apply the inch-pound and SI values independently. They are not exact equivalents.
- [7] Cast test bars separately from the same lot. Use dried, baked or chemically bonded silica-sand molds with suitable binders and similar sand grain size to the casting molds. The molds must be approximately at room temperature when poured, with surrounding sand at least one bar diameter thick.
- [8] When the casting is cooled in the mold below 480 °C before shakeout, cool the test bar in its mold below 480 °C before optional still-air cooling to room temperature. For castings shaken out above 480 °C, either follow that route or, by manufacturer–purchaser agreement, shake out the bar at about the casting temperature.
- [9] If insufficient separately cast test pieces are available, a specimen may be taken from a representative location on a casting by manufacturer–purchaser agreement.
- [10] Informative: If a casting-to-coupon correlation is needed, testing may establish it. If reliable correlation data are unavailable and testing is impracticable, select a test casting approximating the main or controlling casting section.
- [11] Apply the tensile load axially. The standard cites ASTM E 8 for the test method.
- [12] If a casting is stress-relieved, annealed, or otherwise heat-treated, give its representative test bars the same treatment alongside the castings.
- [13] If the first test shows that heat treatment is needed to meet the requirements, treat the entire casting lot and its representative test specimens together, then perform the required testing. After a valid nonconforming test, make two retests and reject the represented castings if either retest fails.
Welding Conditions
ASTM A48/A48M — 03
| Property | Value |
|---|---|
| Post-weld Heat Treatment | Informative: Where practical, suitable post-weld heat treatment may reduce adverse effects of welding on the casting.[1][2] |
Notes
- [1] Informative option after authorized welding repair; The standard prohibits repair by plugging or welding unless the purchaser gives written permission.
- [2] Informative values; not mandatory acceptance limits.
Applications
Gray iron ASTM A48M Class 150 is one grade in the gray iron casting family, which includes castings for machine-tool heads and parts for pumps and compressors. These are family applications. The drawing and service requirements determine the grade for a specific part.
Need Class 150 Castings?
Contact us for casting and machining inquiries.
Email Us for a QuoteLast Updated: November 25, 2026