CE20N is one stainless steel grade which listed in ASTM A351. Casting UNS number is J92802. WWW.CASTINGQUALITY.COM
Casting Methods in Casting Quality Industrial:
- Sand Casting
- Investment Casting (Lost Wax Casting, Precision Casting)
ASTM A351 CE20N (UNS J92802) EquivalentStainless Steel Grade: WWW.CASTINGQUALITY.COM
N/A
Reference Casting Standards and others
ASTM A351 Standard Specification for Castings, Austenitic, for Pressure-Containing Parts.
Our Services
- Sand Casting
Casting Quality focus on Metal Parts industry, we provide professional service in Metal Casting field.
Sand Casting is a popular metal form method, are suitable for all materiel, such as grey iron, ductile iron, malleable iron, carbon steel, stainless steel, aluminum and bronze.
- Investment Casting
also named as precision lost wax casting, mainly suitalbe for carbon steel and stainless steel parts. We also provide grey iron and ductile iron and aluminum and bronze parts by investment casting. It can achieve the best appearance with good tolerance
- Shell Casting
Shell casting method is a good option to replace investment casting and sand casting. the quality is better than sand casting parts, suitable for bulk production.
- CNC Machining
CNC Milling, CNC turning with 5 xix CNC center, we provide precision machining for all castings based on customers design drawings.
- CAD Design
Mechanical Design service based on customers requirement, our software is Solidworks and AutoCAD.
- Tools/Mold Design
Mould design and production will be served for metal casting ad plastic injection industry. Based on our more than 10 years experience, we supply professional molds for our customers in Europe and North American.
Stainless Steel Grade | CE20N Chemical Composition / Physical Properties % (max, except where range is given) | ||||||||||
Standard | Grade | Carbon | Manganese | Silicon | Sulfur | Phosphorus | Chromium | Nickel | Molybdenum | Nitrogen | Iron |
ASTM A351 | CE20N | 0.20 | 1.50 | 1.50 | 0.04 | 0.04 | 23.0-26.0 | 8.0-11.0 | 0.50 | 0.08-0.20 | BAL |
CE20N Heat treatment process: WWW.CASTINGQUALITY.COM
Heat to 2225°F [1220°C] minimum, hold for sufficient time to heat casting to temperature, quench in water.
Or castings may be furnace cooled to 2050°F [1120°C] minimum, held for 15 min minimum and then quenched in water or rapidly cooled by others means.
CE20N Stainless Steel Mechanical Property WWW.CASTINGQUALITY.COM
Stainless Steel Grade | Tensile Strength min | Yield Strength, min | Elongation, min | ||||
Standard | Grade | UNS | Ksi | MPa | Ksi | MPa | % |
ASTM A351 | CE20N | J92802 | 80 | 550 | 40 | 275 | 30.0 |
CE20N Typical Application
- Pump components
- Valve components
- HEAT EXCHANGERS
- WATER SYSTEMS
- OFFSHORE PLATFORMS
- FIRE-FIGHTING SYSTEMS