Introduction
GB/T 1348 Grade QT350-22L is a spheroidal graphite iron casting grade. Process options include sand casting, shell molding and lost-foam casting. Typical uses include pump housings, valve bodies, bearing supports and equipment brackets.
| Field | Value |
|---|---|
| Designation | QT350-22L |
| Material Type | Cast Iron |
| Sub Type | Ductile Cast Iron |
| Product Form | casting |
Manufacturing Process
Sand Casting
Shell Molding Casting
Lost Foam Casting
Equivalent Materials
| Standard | Material Grade |
|---|---|
| EN 1563 | EN-GJS-350-22-LT |
| ISO 1083 | ISO1083/JS/350-22-LT |
Approximate materials; not guaranteed interchangeable.
Similar Materials
Not Available
Reference Standards
| Standard | Standard Title | Edition | Specification |
|---|---|---|---|
| GB/T 1348 | Spheroidal graphite iron castings | 2019 | QT350-22L |
Related Casting Products
Physical Properties
Not Available
Chemical Composition
No specified chemical composition limits in GB/T 1348
Heat Treatment
General casting and chemical requirements — No grade-specific heat-treatment temperature or holding schedule is prescribed. Alloy adjustment or heat treatment may control the ferrite/pearlite ratio (6.2). When heat treatment is required, test blocks receive the same treatment as the represented castings; cast-on blocks remain attached until after heat treatment unless agreed otherwise (8.1.6; 8.2.3.5; 8.2.5.5). Repeated heat treatments for retesting shall not exceed two (10.5.3).
Mechanical Properties
Primary Mechanical Properties
GB/T 1348 — 2019
Condition: Table 1; Separately cast, cast-on or side-by-side cast sample; 30 < t ≤ 60 mm; normative; 30 < t ≤ 60 mm
| Property | Requirement |
|---|---|
| Yield Strength (Rp0.2) | ≥ 210 MPa[1][2][3][4] |
| Tensile Strength | ≥ 330 MPa[1][2][3][4] |
| Elongation | ≥ 18 %[1][2][3][4] |
Notes
- [1] Table 1: results from cast samples do not directly represent casting-body properties. Separately cast, cast-on and side-by-side cast samples are covered. L denotes low temperature and R room temperature. Elongation is measured at original gauge length L0=5d; alternate gauge lengths require the provisions of 9.1 and normative Annex D.
- [2] Gauge Length: L0 = 5d
- [3] GB/T 228.1
- [4] Minimum prescribed value
GB/T 1348 — 2019
Condition: Table 1; Separately cast, cast-on or side-by-side cast sample; 60 < t ≤ 200 mm; normative; 60 < t ≤ 200 mm
| Property | Requirement |
|---|---|
| Yield Strength (Rp0.2) | ≥ 200 MPa[1][2][3][4] |
| Tensile Strength | ≥ 320 MPa[1][2][3][4] |
| Elongation | ≥ 15 %[1][2][3][4] |
Notes
- [1] Table 1: results from cast samples do not directly represent casting-body properties. Separately cast, cast-on and side-by-side cast samples are covered. L denotes low temperature and R room temperature. Elongation is measured at original gauge length L0=5d; alternate gauge lengths require the provisions of 9.1 and normative Annex D.
- [2] Gauge Length: L0 = 5d
- [3] GB/T 228.1
- [4] Minimum prescribed value
GB/T 1348 — 2019
Condition: Table 1; Separately cast, cast-on or side-by-side cast sample; t ≤ 30 mm; normative; t ≤ 30 mm
| Property | Requirement |
|---|---|
| Yield Strength (Rp0.2) | ≥ 220 MPa[1][2][3][4] |
| Tensile Strength | ≥ 350 MPa[1][2][3][4] |
| Elongation | ≥ 22 %[1][2][3][4] |
Notes
- [1] Table 1: results from cast samples do not directly represent casting-body properties. Separately cast, cast-on and side-by-side cast samples are covered. L denotes low temperature and R room temperature. Elongation is measured at original gauge length L0=5d; alternate gauge lengths require the provisions of 9.1 and normative Annex D.
- [2] Gauge Length: L0 = 5d
- [3] GB/T 228.1
- [4] Minimum prescribed value
GB/T 1348 — 2019
Condition: Table C.1; Specimen cut from the casting; source designation QT350-22L/C; sampling position and acceptance properties subject to agreement; 30 < t ≤ 60 mm; informative; 30 < t ≤ 60 mm
Informative
| Property | Value |
|---|---|
| Yield Strength (Rp0.2) | ≥ 210 MPa[1][2][3][4][5][6] |
| Tensile Strength | ≥ 320 MPa[1][2][3][4][5][6] |
| Elongation | ≥ 15 %[1][2][3][4][5][6] |
Notes
- [1] informative 30 < wall thickness ≤ 60 mm
- [2] Gauge Length: L0 = 5d
- [3] GB/T 228.1
- [4] Informative minimum guideline, not an unconditional acceptance requirement
- [5] Informative reference value
- [6] not an acceptance requirement
GB/T 1348 — 2019
Condition: Table C.1; Specimen cut from the casting; source designation QT350-22L/C; sampling position and acceptance properties subject to agreement; 60 < t ≤ 200 mm; informative; 60 < t ≤ 200 mm
Informative
| Property | Value |
|---|---|
| Yield Strength (Rp0.2) | ≥ 200 MPa[1][2][3][4][5][6] |
| Tensile Strength | ≥ 310 MPa[1][2][3][4][5][6] |
| Elongation | ≥ 12 %[1][2][3][4][5][6] |
Notes
- [1] informative 60 < wall thickness ≤ 200 mm
- [2] Gauge Length: L0 = 5d
- [3] GB/T 228.1
- [4] Informative minimum guideline, not an unconditional acceptance requirement
- [5] Informative reference value
- [6] not an acceptance requirement
GB/T 1348 — 2019
Condition: Table C.1; Specimen cut from the casting; source designation QT350-22L/C; sampling position and acceptance properties subject to agreement; t ≤ 30 mm; informative; t ≤ 30 mm
Informative
| Property | Value |
|---|---|
| Yield Strength (Rp0.2) | ≥ 220 MPa[1][2][3][4][5][6] |
| Tensile Strength | ≥ 340 MPa[1][2][3][4][5][6] |
| Elongation | ≥ 20 %[1][2][3][4][5][6] |
Notes
- [1] informative wall thickness ≤ 30 mm
- [2] Gauge Length: L0 = 5d
- [3] GB/T 228.1
- [4] Informative minimum guideline, not an unconditional acceptance requirement
- [5] Informative reference value
- [6] not an acceptance requirement
Additional Mechanical Properties
GB/T 1348 — 2019
Low-Temperature Properties
Condition: Table 2; V-notched specimen machined from separately cast, cast-on or side-by-side cast sample; 30 < t ≤ 60 mm; Mean of three specimens; Test temperature -40 °C; normative; 30 < t ≤ 60 mm; -40
Notes
- [1] Table 2 notes: these grades may also be used for pressure vessels; this does not by itself establish compliance with a vessel design code. Cast-sample properties do not directly represent every part of a casting. Values apply to separately cast, cast-on and side-by-side cast samples. L denotes low temperature and R room temperature. Dashed temperature cells do not prescribe numerical impact requirements.
- [2] normative 30 < wall thickness ≤ 60 mm
- [3] Test temperature tolerance (recorded value): 2
- [4] GB/T 229
- [5] 2 mm striker radius
- [6] Figure 6
- [7] Impact testing only when required by the purchaser (7.2.1.2)
- [8] no requirement at the dashed temperatures
GB/T 1348 — 2019
Low-Temperature Properties
Condition: Table 2; V-notched specimen machined from separately cast, cast-on or side-by-side cast sample; 30 < t ≤ 60 mm; Minimum individual specimen; Test temperature -40 °C; normative; 30 < t ≤ 60 mm; -40
Notes
- [1] Table 2 notes: these grades may also be used for pressure vessels; this does not by itself establish compliance with a vessel design code. Cast-sample properties do not directly represent every part of a casting. Values apply to separately cast, cast-on and side-by-side cast samples. L denotes low temperature and R room temperature. Dashed temperature cells do not prescribe numerical impact requirements.
- [2] normative 30 < wall thickness ≤ 60 mm
- [3] Test temperature tolerance (recorded value): 2
- [4] GB/T 229
- [5] 2 mm striker radius
- [6] Figure 6
- [7] Impact testing only when required by the purchaser (7.2.1.2)
- [8] no requirement at the dashed temperatures
GB/T 1348 — 2019
Low-Temperature Properties
Condition: Table 2; V-notched specimen machined from separately cast, cast-on or side-by-side cast sample; 60 < t ≤ 200 mm; Mean of three specimens; Test temperature -40 °C; normative; 60 < t ≤ 200 mm; -40
Notes
- [1] Table 2 notes: these grades may also be used for pressure vessels; this does not by itself establish compliance with a vessel design code. Cast-sample properties do not directly represent every part of a casting. Values apply to separately cast, cast-on and side-by-side cast samples. L denotes low temperature and R room temperature. Dashed temperature cells do not prescribe numerical impact requirements.
- [2] normative 60 < wall thickness ≤ 200 mm
- [3] Test temperature tolerance (recorded value): 2
- [4] GB/T 229
- [5] 2 mm striker radius
- [6] Figure 6
- [7] Impact testing only when required by the purchaser (7.2.1.2)
- [8] no requirement at the dashed temperatures
GB/T 1348 — 2019
Low-Temperature Properties
Condition: Table 2; V-notched specimen machined from separately cast, cast-on or side-by-side cast sample; 60 < t ≤ 200 mm; Minimum individual specimen; Test temperature -40 °C; normative; 60 < t ≤ 200 mm; -40
Notes
- [1] Table 2 notes: these grades may also be used for pressure vessels; this does not by itself establish compliance with a vessel design code. Cast-sample properties do not directly represent every part of a casting. Values apply to separately cast, cast-on and side-by-side cast samples. L denotes low temperature and R room temperature. Dashed temperature cells do not prescribe numerical impact requirements.
- [2] normative 60 < wall thickness ≤ 200 mm
- [3] Test temperature tolerance (recorded value): 2
- [4] GB/T 229
- [5] 2 mm striker radius
- [6] Figure 6
- [7] Impact testing only when required by the purchaser (7.2.1.2)
- [8] no requirement at the dashed temperatures
GB/T 1348 — 2019
Low-Temperature Properties
Condition: Table 2; V-notched specimen machined from separately cast, cast-on or side-by-side cast sample; t ≤ 30 mm; Mean of three specimens; Test temperature -40 °C; normative; t ≤ 30 mm; -40
Notes
- [1] Table 2 notes: these grades may also be used for pressure vessels; this does not by itself establish compliance with a vessel design code. Cast-sample properties do not directly represent every part of a casting. Values apply to separately cast, cast-on and side-by-side cast samples. L denotes low temperature and R room temperature. Dashed temperature cells do not prescribe numerical impact requirements.
- [2] normative wall thickness ≤ 30 mm
- [3] Test temperature tolerance (recorded value): 2
- [4] GB/T 229
- [5] 2 mm striker radius
- [6] Figure 6
- [7] Impact testing only when required by the purchaser (7.2.1.2)
- [8] no requirement at the dashed temperatures
GB/T 1348 — 2019
Low-Temperature Properties
Condition: Table 2; V-notched specimen machined from separately cast, cast-on or side-by-side cast sample; t ≤ 30 mm; Minimum individual specimen; Test temperature -40 °C; normative; t ≤ 30 mm; -40
Notes
- [1] Table 2 notes: these grades may also be used for pressure vessels; this does not by itself establish compliance with a vessel design code. Cast-sample properties do not directly represent every part of a casting. Values apply to separately cast, cast-on and side-by-side cast samples. L denotes low temperature and R room temperature. Dashed temperature cells do not prescribe numerical impact requirements.
- [2] normative wall thickness ≤ 30 mm
- [3] Test temperature tolerance (recorded value): 2
- [4] GB/T 229
- [5] 2 mm striker radius
- [6] Figure 6
- [7] Impact testing only when required by the purchaser (7.2.1.2)
- [8] no requirement at the dashed temperatures
Welding Conditions
Not Available
Applications
Ductile iron GB/T 1348 Grade QT350-22L is used for pump housings, valve bodies, bearing supports and equipment brackets. These castings are found in fluid-handling equipment, agricultural machinery and general mechanical assemblies. Selection within this family depends on the actual component geometry and loading.
Pipes, pipe fittings and associated joints are outside this standard; pressure-retaining machinery parts require the applicable component specification and inspection requirements. For this suffix grade, retain the specified impact-test temperature and specimen conditions when selecting a component; the test temperature is not a guaranteed operating-temperature limit.
Need QT350-22L Castings?
Contact us for casting and machining inquiries.
Email Us for a QuoteLast Updated: November 25, 2026