Introduction
GB/T 1348 Grade QT-HBW175 is a spheroidal graphite iron casting grade. Process options include sand casting, shell molding and lost-foam casting. Typical uses include machined housings, hubs, gear blanks and general engineering castings.
| Field | Value |
|---|---|
| Designation | QT-HBW175 |
| Material Type | Cast Iron |
| Sub Type | Ductile Cast Iron |
| Product Form | casting |
Manufacturing Process
Sand Casting
Shell Molding Casting
Lost Foam Casting
Equivalent Materials
Not Available
Similar Materials
Not Available
Reference Standards
| Standard | Standard Title | Edition | Specification |
|---|---|---|---|
| GB/T 1348 | Spheroidal graphite iron castings | 2019 | QT-HBW175 |
Related Casting Products
Physical Properties
Not Available
Chemical Composition
No specified chemical composition limits in GB/T 1348
Heat Treatment
General casting and chemical requirements — No grade-specific heat-treatment temperature or holding schedule is prescribed. Alloy adjustment or heat treatment may control the ferrite/pearlite ratio (6.2). When heat treatment is required, test blocks receive the same treatment as the represented castings; cast-on blocks remain attached until after heat treatment unless agreed otherwise (8.1.6; 8.2.3.5; 8.2.5.5). Repeated heat treatments for retesting shall not exceed two (10.5.3).
Mechanical Properties
Primary Mechanical Properties
GB/T 1348 — 2019
Condition: Table E.2; Test bar or agreed position on casting; manufacturer selects a representative casting position in the absence of agreement; informative
Informative
| Property | Value |
|---|---|
| Brinell Hardness | 160–190 HBW[1][2][3][4][5][6] |
| Tensile Strength | ≥ 450 MPa[1][2][3][4][5][7] |
| Yield Strength (Rp0.2) | ≥ 350 MPa[1][2][3][4][5][7] |
Notes
- [1] informative Test bar or agreed position on casting
- [2] Annex E applies only by agreement. Tensile/proof strength values are reference data when hardness is the inspection characteristic. QT-HBW300 and QT-HBW330 are not applicable to thick-walled castings. Hardness testing frequency and number are agreed
- [3] E.3 procedure applies when hardness and tensile properties are both specified.
- [4] Informative reference value
- [5] not an acceptance requirement
- [6] Brinell Hardness: GB/T 231.1
- [7] Tensile Strength; Yield Strength (Rp0.2): Reference only
Welding Conditions
Not Available
Applications
Ductile iron GB/T 1348 Grade QT-HBW175 is used for machined housings, hubs, gear blanks and general engineering castings. This designation is selected by its specified hardness requirements rather than by assuming a particular tensile grade. The intended component must therefore be checked against the agreed hardness range and any additional mechanical requirements.
Family-level examples do not establish a grade-specific pressure, impact or fatigue rating.
Need QT-HBW175 Castings?
Contact us for casting and machining inquiries.
Email Us for a QuoteLast Updated: November 25, 2026