ISO1083/JS/450-10 Ductile Cast Iron Casting Material
Ductile Cast Iron
Introduction
ISO1083/JS/450-10 is an ISO 1083 grade of spheroidal graphite cast iron. The standard reports ferrite as a typical matrix. Family applications include hubs and gears in agricultural and industrial machinery.
| Field | Value |
|---|---|
| Designation | ISO1083/JS/450-10 |
| Material Type | Cast Iron |
| Sub Type | Ductile Cast Iron |
| Product Form | casting |
Manufacturing Process
Sand Casting
Shell Molding Casting
Lost Foam Casting
Equivalent Materials
Approximate materials; not guaranteed interchangeable.
Similar Materials
Not Available
Reference Standards
| Standard | Standard Title | Edition | Specification |
|---|---|---|---|
| ISO 1083 | Spheroidal graphite cast irons — Classification | 2018 | ISO1083/JS/450-10 |
Related Casting Products
Physical Properties
| Property | Value | Applicable Conditions |
|---|---|---|
| Density | 7.1 kg/dm³[2] | Room temperature unless otherwise specified |
| Elastic Modulus | 169 GN/m²[2] | Room temperature unless otherwise specified |
| Poisson Ratio | 0.275[2] | Room temperature unless otherwise specified |
| Thermal Conductivity | 36.2 W/(m·K)[2] | Test temperature: 300 °C |
| Specific Heat | 515 J/(kg·K)[2] | Temperature range: 20–500 °C |
| Thermal Expansion | 12.5 µm/(m·K)[2] | Temperature range: 20–400 °C |
| Electrical Resistivity | 0.50 µΩ·m[2] | Room temperature unless otherwise specified |
| Hysteresis Loss | 600 J/m³[2] | Hysteresis loss at B = 1 T; Room temperature unless otherwise specified |
| Matrix Structure | ferrite[1][2] | |
| Maximum Magnetic Permeability | 2136 µH/m[2] | Room temperature unless otherwise specified |
Notes
- [1] Matrix Structure: Typical structure
- [2] Informative values; not mandatory acceptance limits.
Chemical Composition
Not Available
Heat Treatment
ISO 1083–2018
Not Available
Mechanical Properties
Primary Mechanical Properties
ISO 1083 — 2018
Condition: t ≤ 30 mm
| Property | Requirement |
|---|---|
| Yield Strength (Rp0.2) | ≥ 310 MPa[1][2][3] |
| Tensile Strength | ≥ 450 MPa[1][2][3] |
| Elongation | ≥ 10 %[1][2][3][4][5] |
Notes
- [1] Separately cast, cast-on or side-by-side cast samples
- [2] Values apply to sand moulds or moulds of comparable thermal behaviour
- [3] alternative processes are subject to amendments agreed in the order.
- [4] Elongation: Elongation values determined from L0 = 5 d
- [5] Elongation: other gauge lengths see 9.1 and Annex B.
ISO 1083 — 2018
Condition: t ≤ 30 mm
Informative
| Property | Value |
|---|---|
| Yield Strength (Rp0.2) | ≥ 300 MPa[1][2][3] |
| Tensile Strength | ≥ 440 MPa[1][2][3] |
| Elongation | ≥ 8 %[1][2][3][4] |
Notes
- [1] test pieces machined from samples cut from castings
- [2] Informative reference value
- [3] not an acceptance requirement
- [4] Elongation: For elongation results, the reference gauge length is L0 = 5 d.
ISO 1083 — 2018
Informative
Notes
- [1] Room temperature unless otherwise specified.
- [2] Informative reference value
- [3] not an acceptance requirement
Additional Mechanical Properties
ISO 1083 — 2018
Other Mechanical Properties
Informative
Notes
- [1] Room temperature unless otherwise specified.
- [2] Informative reference value
- [3] not an acceptance requirement
ISO 1083 — 2018
Fatigue Properties
Informative
| Property | Value |
|---|---|
| Reversed Tension Compression Fatigue Strength | 185 MPa[1][2][3][4][5][6] |
| Reversed Tension Compression Fatigue Ratio | 0.41[1][2][3][4][5][6] |
| Pulsating Tension Fatigue Strength | 259 MPa[1][2][3][4][5][6] |
| Reversed Torsional Fatigue Strength | 166 MPa[1][2][3][4][5][6] |
| Reversed Torsional Fatigue Ratio | 0.37[1][2][3][4][5][6] |
| Rotating Bending Fatigue Strength | 207 MPa[1][2][3][4][5][6] |
| Rotating Bending Fatigue Ratio | 0.46[1][2][3][4][5][6] |
| Notched Rotating Bending Fatigue Strength | 139 MPa[1][2][4][5][6][7] |
| Notched Rotating Bending Fatigue Ratio | 0.31[1][2][4][5][6][7] |
Notes
- [1] specimens diameter <=25 mm from casting
- [2] relevant wall thickness <=30 mm
- [3] Reversed Tension Compression Fatigue Strength; Reversed Tension Compression Fatigue Ratio; Pulsating Tension Fatigue Strength; Reversed Torsional Fatigue Strength; Reversed Torsional Fatigue Ratio; Rotating Bending Fatigue Strength; Rotating Bending Fatigue Ratio: Unnotched specimen
- [4] 10 million cycles and 50% failure probability.
- [5] Informative reference value
- [6] not an acceptance requirement
- [7] Notched Rotating Bending Fatigue Strength; Notched Rotating Bending Fatigue Ratio: Notched specimen with stress concentration factor Kt ≤ 3
Welding Conditions
Not Available
Applications
Ductile iron ISO1083/JS/450-10 belongs to the spheroidal graphite iron casting family. Ductile-iron foundries make gears, hubs and brackets alongside pump casings and bearing housings for engineering equipment. Manufacturers supply such castings for agricultural equipment, vehicle assemblies and flow-control machinery.
Need ISO1083/JS/450-10 Castings?
Contact us for casting and machining inquiries.
Email Us for a QuoteLast Updated: November 16, 2026