ISO1083/JS/400-18 Ductile Cast Iron Casting Material
Ductile Cast Iron
Introduction
ISO1083/JS/400-18 is a spheroidal graphite iron casting material in ISO 1083. The standard reports ferrite as a typical matrix. The wider ductile-iron family is used for pump casings and machinery housings.
| Field | Value |
|---|---|
| Designation | ISO1083/JS/400-18 |
| Material Type | Cast Iron |
| Sub Type | Ductile Cast Iron |
| Product Form | casting |
Manufacturing Process
Sand Casting
Shell Molding Casting
Lost Foam Casting
Equivalent Materials
Approximate materials; not guaranteed interchangeable.
Similar Materials
Not Available
Reference Standards
| Standard | Standard Title | Edition | Specification |
|---|---|---|---|
| ISO 1083 | Spheroidal graphite cast irons — Classification | 2018 | ISO1083/JS/400-18 |
Related Casting Products
Physical Properties
| Property | Value | Applicable Conditions |
|---|---|---|
| Density | 7.1 kg/dm³[2] | Room temperature unless otherwise specified |
| Elastic Modulus | 169 GN/m²[2] | Room temperature unless otherwise specified |
| Poisson Ratio | 0.275[2] | Room temperature unless otherwise specified |
| Thermal Conductivity | 36.2 W/(m·K)[2] | Test temperature: 300 °C |
| Specific Heat | 515 J/(kg·K)[2] | Temperature range: 20–500 °C |
| Thermal Expansion | 12.5 µm/(m·K)[2] | Temperature range: 20–400 °C |
| Electrical Resistivity | 0.50 µΩ·m[2] | Room temperature unless otherwise specified |
| Hysteresis Loss | 600 J/m³[2] | Hysteresis loss at B = 1 T; Room temperature unless otherwise specified |
| Matrix Structure | ferrite[1][2] | |
| Maximum Magnetic Permeability | 2136 µH/m[2] | Room temperature unless otherwise specified |
Notes
- [1] Matrix Structure: Typical structure
- [2] Informative values; not mandatory acceptance limits.
Chemical Composition
Not Available
Heat Treatment
ISO 1083–2018
Not Available
Mechanical Properties
Primary Mechanical Properties
ISO 1083 — 2018
| Property | t ≤ 30 mm | 30 < t ≤ 60 mm | 60 < t ≤ 200 mm |
|---|---|---|---|
| Yield Strength (Rp0.2) | ≥ 250 MPa[1][2][3] | ≥ 250 MPa[1][2][3] | ≥ 240 MPa[1][2][3] |
| Tensile Strength | ≥ 400 MPa[1][2][3] | ≥ 390 MPa[1][2][3] | ≥ 370 MPa[1][2][3] |
| Elongation | ≥ 18 %[1][2][3][4][5] | ≥ 15 %[1][2][3][4][5] | ≥ 12 %[1][2][3][4][5] |
Notes
- [1] Separately cast, cast-on or side-by-side cast samples
- [2] Values apply to sand moulds or moulds of comparable thermal behaviour
- [3] alternative processes are subject to amendments agreed in the order.
- [4] Elongation: Elongation values determined from L0 = 5 d
- [5] Elongation: other gauge lengths see 9.1 and Annex B.
ISO 1083 — 2018
Informative
| Property | t ≤ 30 mm | 30 < t ≤ 60 mm | 60 < t ≤ 200 mm |
|---|---|---|---|
| Yield Strength (Rp0.2) | ≥ 250 MPa[1][2][3] | ≥ 240 MPa[1][2][3] | ≥ 230 MPa[1][2][3] |
| Tensile Strength | ≥ 390 MPa[1][2][3] | ≥ 370 MPa[1][2][3] | ≥ 350 MPa[1][2][3] |
| Elongation | ≥ 15 %[1][2][3][4] | ≥ 12 %[1][2][3][4] | ≥ 10 %[1][2][3][4] |
Notes
- [1] test pieces machined from samples cut from castings
- [2] Informative reference value
- [3] not an acceptance requirement
- [4] Elongation: For elongation results, the reference gauge length is L0 = 5 d.
ISO 1083 — 2018
Informative
Notes
- [1] Room temperature unless otherwise specified.
- [2] Informative reference value
- [3] not an acceptance requirement
Additional Mechanical Properties
ISO 1083 — 2018
Other Mechanical Properties
Informative
Notes
- [1] Room temperature unless otherwise specified.
- [2] Informative reference value
- [3] not an acceptance requirement
ISO 1083 — 2018
Fatigue Properties
Informative
| Property | Value |
|---|---|
| Reversed Tension Compression Fatigue Strength | 168 MPa[1][2][3][4][5][6] |
| Reversed Tension Compression Fatigue Ratio | 0.42[1][2][3][4][5][6] |
| Pulsating Tension Fatigue Strength | 235 MPa[1][2][3][4][5][6] |
| Reversed Torsional Fatigue Strength | 152 MPa[1][2][3][4][5][6] |
| Reversed Torsional Fatigue Ratio | 0.38[1][2][3][4][5][6] |
| Rotating Bending Fatigue Strength | 188 MPa[1][2][3][4][5][6] |
| Rotating Bending Fatigue Ratio | 0.47[1][2][3][4][5][6] |
| Notched Rotating Bending Fatigue Strength | 128 MPa[1][2][4][5][6][7] |
| Notched Rotating Bending Fatigue Ratio | 0.32[1][2][4][5][6][7] |
Notes
- [1] specimens diameter <=25 mm from casting
- [2] relevant wall thickness <=30 mm
- [3] Reversed Tension Compression Fatigue Strength; Reversed Tension Compression Fatigue Ratio; Pulsating Tension Fatigue Strength; Reversed Torsional Fatigue Strength; Reversed Torsional Fatigue Ratio; Rotating Bending Fatigue Strength; Rotating Bending Fatigue Ratio: Unnotched specimen
- [4] 10 million cycles and 50% failure probability.
- [5] Informative reference value
- [6] not an acceptance requirement
- [7] Notched Rotating Bending Fatigue Strength; Notched Rotating Bending Fatigue Ratio: Notched specimen with stress concentration factor Kt ≤ 3
Welding Conditions
Not Available
Applications
Ductile iron ISO1083/JS/400-18 belongs to the spheroidal graphite iron casting family. Foundry applications for spheroidal graphite iron include gears, support brackets, wheel hubs and casings for industrial pumps. These types of components occur in agricultural machinery, construction equipment and industrial fluid-handling systems.