GGG-35.3 (EN 0.7033) Ductile Cast Iron Casting Material
Ductile Cast Iron
Introduction
DIN 1693-1 Grade GGG-35.3 is a ductile cast iron grade. Process options include sand casting, shell molding and lost-foam casting. Typical family applications include gear and transmission components, hubs, brackets, machine housings and pump-related castings.
| Field | Value |
|---|---|
| Designation | GGG-35.3 (EN 0.7033) |
| Material Type | Cast Iron |
| Sub Type | Ductile Cast Iron |
| Product Form | casting |
Manufacturing Process
Sand Casting
Shell Molding Casting
Lost Foam Casting
Equivalent Materials
Not Available
Similar Materials
Not Available
Reference Standards
| Standard | Standard Title | Edition | Specification | Identifier |
|---|---|---|---|---|
| DIN 1693-1 | Cast Iron with Nodular Graphite — Unalloyed and Low Alloy Grades | 1973-10 | GGG-35.3 | DIN 0.7033 |
Related Casting Products
Physical Properties
Chemical Composition
Notes
- [1] Explanations: manufacturing aim for GGG-35.3, informative only; P is strictly less than 0.05 %, not a general mandatory acceptance maximum.; Explanatory manufacturing aim only; P <0.05 % (strict inequality). Do not treat these as normative chemistry limits.
- [2] Informative values; not mandatory acceptance limits.
Heat Treatment
Separately cast test piece — GGG-35.3 must be annealed to give a ferritic condition.
Mechanical Properties
Primary Mechanical Properties
DIN 1693-1 — 1973-10
Condition: Separately cast test piece
| Property | Requirement |
|---|---|
| Tensile Strength | ≥ 350 N/mm²[1][2][3][4] |
| Yield Strength (Rp0.2) | ≥ 220 N/mm²[1][2][3][4] |
| Elongation | ≥ 22 %[1][2][3][4] |
Notes
- [1] Specimen dimensions and number are agreed; otherwise manufacturer decides. Test-piece thickness should approximate ruling casting thickness. For sections >50 mm and compact castings, agreement is urged; these are separately cast test-piece guarantees, not universal casting-location minima.
- [2] Separately cast U or Y test piece
- [3] tensile specimen per DIN 50125
- [4] A5 elongation
DIN 1693-1 — 1973-10
Condition: room temperature; no numeric temperature invented; Separately cast test piece
| Property | Mean of 3 DVM specimens | Individual DVM specimen |
|---|---|---|
| Impact Energy (DVM) | ≥ 19 J[1][2][3] | ≥ 17 J[2][3][4] |
Notes
- [1] Impact Energy (DVM) [Mean of 3 DVM specimens]: DVM specimens; not a Charpy V-notch conversion. Mean of 3 DVM specimens
- [2] DVM notched-bar impact specimen per DIN 50115
- [3] Condition: Separately cast test piece
- [4] Impact Energy (DVM) [Individual DVM specimen]: DVM specimens; not a Charpy V-notch conversion. Individual DVM specimen
Additional Mechanical Properties
DIN 1693-1 — 1973-10
Low-Temperature Properties
Condition: -40 °C; Separately cast test piece
| Property | Mean of 3 DVM specimens | Individual DVM specimen |
|---|---|---|
| Impact Energy (DVM) | ≥ 14 J[1][2][3] | ≥ 11 J[2][3][4] |
Notes
- [1] Impact Energy (DVM) [Mean of 3 DVM specimens]: DVM specimens; not a Charpy V-notch conversion. Mean of 3 DVM specimens
- [2] DVM notched-bar impact specimen per DIN 50115
- [3] Condition: Separately cast test piece
- [4] Impact Energy (DVM) [Individual DVM specimen]: DVM specimens; not a Charpy V-notch conversion. Individual DVM specimen
Welding Conditions
Not Available
Applications
For ductile cast iron DIN 1693-1 GGG-35.3, typical cast components in this material family include gear and transmission components, hubs, brackets, machine housings and pump-related castings. Applications include agricultural, construction and general industrial machinery. Lifting, low-temperature and pressure-retaining duties require the relevant component-specific requirements; ordinary family uses do not establish those capabilities.
Need GGG-35.3 Castings?
Contact us for casting and machining inquiries.
Email Us for a QuoteLast Updated: November 25, 2026