Introduction
ASTM A128/A128M Grade A is an austenitic manganese steel casting grade. It is the default grade unless another is specified. The specification defines its composition and heat treatment for castings.
| Field | Value |
|---|---|
| Designation | A |
| Material Type | Alloy Steel |
| Sub Type | High-Alloy Steel |
| Product Form | casting |
Manufacturing Process
Investment Casting
Shell Molding Casting
Sand Casting
Equivalent Materials
Not Available
Similar Materials
Not Available
Reference Standards
| Standard | Standard Title | Edition | Specification |
|---|---|---|---|
| ASTM A128/A128M | Steel Castings, Austenitic Manganese | 93(2003) | A |
Related Casting Products
Physical Properties
Not Available
Chemical Composition
| Element | Requirement |
|---|---|
| C | 1.05–1.35 % |
| Si | ≤ 1.00 % |
| Mn | ≥ 11.0 % |
| P | ≤ 0.07 % |
Heat Treatment
| Heat Treatment | Operation | Temperature | Holding Time | Cooling |
|---|---|---|---|---|
| Default delivery heat treatment | heat treatment[1] | ≥ 1800°F [1000°C] | Hold until the temperature is uniform throughout the casting. | Quench in a suitable medium, normally water |
Notes
- [1] A different delivery condition may be used by agreement between the purchaser and manufacturer.
Mechanical Properties
Additional Mechanical Properties
ASTM A128/A128M — 93(2003)
Other Mechanical Properties
Condition: Supplementary S50, only when specified
Notes
- [1] When S50 is specified, test one specimen from each heat. Cold-bend it around a 1 in. [25.4 mm] pin without breaking it into two pieces. Surface cracks alone are acceptable if it remains in one piece. Cast specimens separately from the same heat in a 1/2 × 3/4 in. [13 × 19 mm] section, 12 in. [300 mm] long. Heat treat and test without machining or grinding except to remove surface irregularities or decarburization. Use the same heat treatment as for the casting, considering section size. Unless the purchaser specifies otherwise, the manufacturer may treat the specimens separately or with the castings. Reheat treatment and retest may be repeated at most twice. After reheating, perform two bend tests per heat. The source note does not recommend this test for the special alloy grades.
- [2] Applies only when Supplementary Requirement S50 is specified
Welding Conditions
ASTM A128/A128M — 93(2003)
| Property | Requirement |
|---|---|
| Weld Repair Deposit | Weld deposits are generally austenitic steel. On wearing surfaces use austenitic manganese steel weld metal.[1] |
Notes
- [1] Use welding procedures and welders capable of producing sound welds. Apply the same inspection quality standards as for the castings.
Applications
Austenitic manganese steel ASTM A128/A128M Grade A belongs to a family used for crusher jaws, cone liners and excavating wear castings. For crushing and digging service, select the casting grade against the section size and expected impact loading.