ISO1083/JS/550-5 Ductile Cast Iron Casting Material
Ductile Cast Iron
Introduction
ISO1083/JS/550-5 is an ISO 1083 ductile iron for castings. The standard reports ferrite-pearlite as a typical matrix. Family applications include hubs and gears in agricultural and industrial machinery.
| Field | Value |
|---|---|
| Designation | ISO1083/JS/550-5 |
| Material Type | Cast Iron |
| Sub Type | Ductile Cast Iron |
| Product Form | casting |
Manufacturing Process
Sand Casting
Shell Molding Casting
Lost Foam Casting
Equivalent Materials
Approximate materials; not guaranteed interchangeable.
Similar Materials
Not Available
Reference Standards
| Standard | Standard Title | Edition | Specification |
|---|---|---|---|
| ISO 1083 | Spheroidal graphite cast irons — Classification | 2018 | ISO1083/JS/550-5 |
Related Casting Products
Physical Properties
| Property | Value | Applicable Conditions |
|---|---|---|
| Density | 7.1 kg/dm³[2] | Room temperature unless otherwise specified |
| Elastic Modulus | 172 GN/m²[2] | Room temperature unless otherwise specified |
| Poisson Ratio | 0.275[2] | Room temperature unless otherwise specified |
| Thermal Conductivity | 34 W/(m·K)[2] | Test temperature: 300 °C |
| Specific Heat | 515 J/(kg·K)[2] | Temperature range: 20–500 °C |
| Thermal Expansion | 12.5 µm/(m·K)[2] | Temperature range: 20–400 °C |
| Electrical Resistivity | 0.52 µΩ·m[2] | Room temperature unless otherwise specified |
| Hysteresis Loss | 1800 J/m³[2] | Hysteresis loss at B = 1 T; Room temperature unless otherwise specified |
| Matrix Structure | ferrite-pearlite[1][2] | |
| Maximum Magnetic Permeability | 1200 µH/m[2] | Room temperature unless otherwise specified |
Notes
- [1] Matrix Structure: Typical structure
- [2] Informative values; not mandatory acceptance limits.
Chemical Composition
Not Available
Heat Treatment
ISO 1083–2018
Not Available
Mechanical Properties
Primary Mechanical Properties
ISO 1083 — 2018
| Property | t ≤ 30 mm | 30 < t ≤ 60 mm | 60 < t ≤ 200 mm |
|---|---|---|---|
| Yield Strength (Rp0.2) | ≥ 350 MPa[1][2][3] | ≥ 330 MPa[1][2][3] | ≥ 320 MPa[1][2][3] |
| Tensile Strength | ≥ 550 MPa[1][2][3] | ≥ 520 MPa[1][2][3] | ≥ 500 MPa[1][2][3] |
| Elongation | ≥ 5 %[1][2][3][4][5] | ≥ 4 %[1][2][3][4][5] | ≥ 3 %[1][2][3][4][5] |
Notes
- [1] Separately cast, cast-on or side-by-side cast samples
- [2] Values apply to sand moulds or moulds of comparable thermal behaviour
- [3] alternative processes are subject to amendments agreed in the order.
- [4] Elongation: Elongation values determined from L0 = 5 d
- [5] Elongation: other gauge lengths see 9.1 and Annex B.
ISO 1083 — 2018
Informative
| Property | t ≤ 30 mm | 30 < t ≤ 60 mm | 60 < t ≤ 200 mm |
|---|---|---|---|
| Yield Strength (Rp0.2) | ≥ 330 MPa[1][2][3] | ≥ 310 MPa[1][2][3] | ≥ 290 MPa[1][2][3] |
| Tensile Strength | ≥ 530 MPa[1][2][3] | ≥ 500 MPa[1][2][3] | ≥ 450 MPa[1][2][3] |
| Elongation | ≥ 4 %[1][2][3][4] | ≥ 3 %[1][2][3][4] | ≥ 2 %[1][2][3][4] |
Notes
- [1] test pieces machined from samples cut from castings
- [2] Informative reference value
- [3] not an acceptance requirement
- [4] Elongation: For elongation results, the reference gauge length is L0 = 5 d.
Welding Conditions
Not Available
Applications
Ductile iron ISO1083/JS/550-5 belongs to the spheroidal graphite iron casting family. In this casting family, components include pump and valve bodies, bearing housings, cover plates and parts for power transmission. Manufacturers supply such castings for agricultural equipment, vehicle assemblies and flow-control machinery.