ISO1083/JS/350-22-RT Ductile Cast Iron Casting Material

Ductile Cast Iron

Download MDS PDF · Request a Quote

Introduction

ISO1083/JS/350-22-RT is a ductile iron casting grade covered by ISO 1083. Its graphite is mainly spheroidal, in forms V and VI. The wider ductile-iron family is used for pump casings and machinery housings. Impact properties apply when testing is specified at order acceptance.

FieldValue
DesignationISO1083/JS/350-22-RT
Material TypeCast Iron
Sub TypeDuctile Cast Iron
Product Formcasting

Manufacturing Process

Sand Casting
Shell Molding Casting
Lost Foam Casting

Equivalent Materials

StandardMaterial Grade
EN 1563EN-GJS-350-22-RT
GB/T 1348QT350-22R

Approximate materials; not guaranteed interchangeable.

Similar Materials

Not Available

Reference Standards

StandardStandard TitleEditionSpecification
ISO 1083Spheroidal graphite cast irons — Classification2018ISO1083/JS/350-22-RT

Physical Properties

Not Available

Chemical Composition

Not Available

Heat Treatment

ISO 1083–2018

Not Available

Mechanical Properties

Primary Mechanical Properties

ISO 1083 — 2018

Condition: Castings-cut specimen, 30 < t ≤ 60; 30 < t ≤ 60 mm

Informative

PropertyValue
Yield Strength (Rp0.2)≥ 210 MPa[1][2][3][4][5][6]
Tensile Strength≥ 320 MPa[1][2][3][4][5][6]
Elongation≥ 15 %[1][2][3][4][5][6][7]

Notes

  • [1] Test pieces machined from samples cut from castings
  • [2] ISO1083/JS/350-22C-RT/C
  • [3] Project owner confirmed mapping to ISO1083/JS/350-22-RT and /C sample-cut-from-casting meaning
  • [4] original source designation retained.
  • [5] Informative reference value
  • [6] not an acceptance requirement
  • [7] Elongation: For elongation results, the reference gauge length is L0 = 5 d.

ISO 1083 — 2018

Condition: Castings-cut specimen, 60 < t ≤ 200; 60 < t ≤ 200 mm

Informative

PropertyValue
Yield Strength (Rp0.2)≥ 200 MPa[1][2][3][4][5][6]
Tensile Strength≥ 310 MPa[1][2][3][4][5][6]
Elongation≥ 12 %[1][2][3][4][5][6][7]

Notes

  • [1] Test pieces machined from samples cut from castings
  • [2] ISO1083/JS/350-22C-RT/C
  • [3] Project owner confirmed mapping to ISO1083/JS/350-22-RT and /C sample-cut-from-casting meaning
  • [4] original source designation retained.
  • [5] Informative reference value
  • [6] not an acceptance requirement
  • [7] Elongation: For elongation results, the reference gauge length is L0 = 5 d.

ISO 1083 — 2018

Condition: Castings-cut specimen, t ≤ 30; t ≤ 30 mm

Informative

PropertyValue
Yield Strength (Rp0.2)≥ 220 MPa[1][2][3][4][5][6]
Tensile Strength≥ 340 MPa[1][2][3][4][5][6]
Elongation≥ 20 %[1][2][3][4][5][6][7]

Notes

  • [1] Test pieces machined from samples cut from castings
  • [2] ISO1083/JS/350-22C-RT/C
  • [3] Project owner confirmed mapping to ISO1083/JS/350-22-RT and /C sample-cut-from-casting meaning
  • [4] original source designation retained.
  • [5] Informative reference value
  • [6] not an acceptance requirement
  • [7] Elongation: For elongation results, the reference gauge length is L0 = 5 d.

ISO 1083 — 2018

Propertyt ≤ 30 mm30 < t ≤ 60 mm60 < t ≤ 200 mm
Yield Strength (Rp0.2)≥ 220 MPa[1][2][3]≥ 220 MPa[1][2][3]≥ 210 MPa[1][2][3]
Tensile Strength≥ 350 MPa[1][2][3]≥ 330 MPa[1][2][3]≥ 320 MPa[1][2][3]
Elongation≥ 22 %[1][2][3][4][5]≥ 18 %[1][2][3][4][5]≥ 15 %[1][2][3][4][5]

Notes

  • [1] Values apply to sand moulds or moulds of comparable thermal behaviour
  • [2] alternative processes are subject to amendments agreed in the order.
  • [3] Separately cast, cast-on or side-by-side cast samples
  • [4] Elongation: Elongation values determined from L0 = 5 d
  • [5] Elongation: other gauge lengths see 9.1 and Annex B.

ISO 1083 — 2018

Condition: mean of three; 23 ± 5 °C

Propertyt ≤ 30 mm30 < t ≤ 60 mm60 < t ≤ 200 mm
Impact Energy≥ 17 J[1][2][3][4][5][6]≥ 17 J[1][2][3][4][5][6]≥ 15 J[1][2][3][4][5][6]

Notes

  • [1] Values apply to sand moulds or moulds of comparable thermal behaviour
  • [2] alternative processes are subject to amendments agreed in the order.
  • [3] V-notched
  • [4] machined from cast samples
  • [5] Mean of three
  • [6] Impact energy is determined only if specified by the purchaser by acceptance of the order.

ISO 1083 — 2018

Condition: individual minimum; 23 ± 5 °C

Propertyt ≤ 30 mm30 < t ≤ 60 mm60 < t ≤ 200 mm
Impact Energy≥ 14 J[1][2][3][4][5][6]≥ 14 J[1][2][3][4][5][6]≥ 12 J[1][2][3][4][5][6]

Notes

  • [1] Values apply to sand moulds or moulds of comparable thermal behaviour
  • [2] alternative processes are subject to amendments agreed in the order.
  • [3] V-notched
  • [4] machined from cast samples
  • [5] Individual minimum
  • [6] Impact energy is determined only if specified by the purchaser by acceptance of the order.

Welding Conditions

Not Available

Applications

Ductile iron ISO1083/JS/350-22-RT belongs to the spheroidal graphite iron casting family. Family-level examples include cast valve bodies, pump housings, bearing housings and covers used in mechanical assemblies. These types of components occur in agricultural machinery, construction equipment and industrial fluid-handling systems. ISO 1083 notes that this grade can be suitable for some pressure-vessel applications; the relevant component requirements still apply.

Need ISO1083/JS/350-22-RT Castings?

Contact us for casting and machining inquiries.

Last Updated: November 16, 2026

error: Alert: Thanks for your interesting, but Article is protected ! You can click the Top Right email!