GX40CrSi17 (EN 1.4740) Ferritic Stainless Steel Casting Material

Ferritic Stainless Steel

Download MDS PDF · Request a Quote

Introduction

EN 10295 Grade GX40CrSi17 is a heat-resistant ferritic stainless steel casting grade. Process options include investment casting, shell molding and sand casting. Typical uses include furnace clamps, brackets and grates.

FieldValue
DesignationGX40CrSi17 (EN 1.4740)
Material TypeStainless Steel
Sub TypeFerritic Stainless Steel
Product Formcasting

Manufacturing Process

Investment Casting
Shell Molding Casting
Sand Casting

Equivalent Materials

Not Available

Similar Materials

Not Available

Reference Standards

StandardStandard TitleEditionSpecificationIdentifier
EN 10295Heat resistant steel castings2002GX40CrSi17EN 1.4740

Physical Properties

PropertyValueApplicable Conditions
Density7.7 kg/dm³[1]
Thermal Conductivity20 W/(m·K)[1]Test temperature: 100 °C
Specific Heat460 J/(kg·K)[1]Test temperature: 20 °C
Thermal Expansion12.5 ×10⁻⁶/K[1]Temperature range: 20–400 °C
Thermal Expansion13.5 ×10⁻⁶/K[1]Temperature range: 20–800 °C

Notes

  • [1] Informative values; not mandatory acceptance limits.

Chemical Composition

ElementRequirement
C0.30–0.50 %[1]
Si1.00–2.50 %[1]
Mn≤ 1.00 %[1]
P≤ 0.040 %[1]
S≤ 0.030 %[1]
Cr16.00–19.00 %[1]
Ni≤ 1.00 %[1]
Mo≤ 0.50 %[1]
Cu≤ 0.20 %[2]
V≤ 0.08 %[2]
Nb≤ 0.20 %[2]
W≤ 0.20 %[2]
Co≤ 0.50 %[2]

Notes

  • [1] C; Si; Mn; P; S; Cr; Mo; Ni: cast analysis
  • [2] W; Nb; V; Cu; Co: Unless otherwise agreed: limit for element unspecified in Table 1; no intentional addition except for finishing the heat.; cast analysis

Heat Treatment

Heat TreatmentOperationTemperature
+Aanneal800–850 °C

Mechanical Properties

Additional Mechanical Properties

EN 10295 — 2002

Creep & Stress-Rupture Properties

Condition: 10000 h

Informative

Property600 °C700 °C800 °C900 °C
σ1% — mean stress for 1% elongation22 MPa[1][2][3][4]9 MPa[1][2][3][4]3.5 MPa[1][2][3][4]1 MPa[1][2][3][4]

Notes

  • [1] Mean creep values from a scatter band of ±20%; information only.
  • [2] Mean values
  • [3] ±20% scatter band
  • [4] information only, not acceptance requirements

EN 10295–2002 · +A

Not Available

Welding Conditions

EN 10295 — 2002

PropertyValue
Preheat300–500 °C[1][2][4]
Post-weld Heat TreatmentStress relief annealing at 760 °C to 800 °C[3][4]

Notes

  • [1] Preheat: The welded area should not cool below the minimum preheat temperature before post-weld heat treatment.
  • [2] Preheat: Production welding; informative Annex A; The welded area should not cool below the minimum preheat temperature before post-weld heat treatment.
  • [3] Post-weld Heat Treatment: Production welding; informative Annex A
  • [4] Informative values; not mandatory acceptance limits.

Applications

Ferritic stainless steel EN 10295 GX40CrSi17 is typically used for furnace clamps, brackets and grates. EN 10295:2002 gives an informative maximum use temperature in air of 900 °C, based on oxidation resistance in clean natural air. These figures are not guaranteed continuous or intermittent service temperatures, or allowable temperatures under load; other atmospheres require separate assessment.

Other cast components used in this material family include furnace fixtures, support elements and burner-assembly components. These applications include industrial heating and heat-treatment equipment. Atmosphere, loading, direct flame exposure, cyclic operation and process deposits must be considered separately from an in-air reference temperature.