GX40CrNiSi25-20 (EN 1.4848) Austenitic Stainless Steel Casting Material
Austenitic Stainless Steel
Introduction
GX40CrNiSi25-20 (EN 1.4848) is an austenitic heat-resistant steel casting grade covered by EN 10295. Casting process options include Investment Casting, Shell Molding Casting, Sand Casting, subject to the applicable specification and component requirements.
| Field | Value |
|---|---|
| Designation | GX40CrNiSi25-20 (EN 1.4848) |
| Material Type | Stainless Steel |
| Sub Type | Austenitic Stainless Steel |
| Product Form | casting |
Manufacturing Process
Investment Casting
Shell Molding Casting
Sand Casting
Equivalent Grades
Similar Materials
N/A
Reference Standards
| Standard | Standard Title | Edition | Specification | Identifier |
|---|---|---|---|---|
| EN 10295 | Heat resistant steel castings | 2002 | GX40CrNiSi25-20 | — |
Related Casting Products
Physical Properties
N/A
Chemical Composition
| Element | EN 10295Edition 2002 · wt.%Cast analysis |
|---|---|
| C | 0.30–0.50 |
| Si | 1.00–2.50 |
| Mn | ≤ 2.00 |
| P | ≤ 0.040 |
| S | ≤ 0.030 |
| Cr | 24.00–27.00 |
| Ni | 19.00–22.00 |
| Mo | ≤ 0.50 |
| Cu | ≤ 0.25[1] |
| Nb | ≤ 0.60[1] |
| V | ≤ 0.12[1] |
| W | ≤ 0.60[1] |
| Co | ≤ 1.00[1] |
Notes
EN 10295 · Edition 2002
[1] Cu/Nb/V/W/Co: Unless otherwise agreed: limit for element unspecified in; no intentional addition except for finishing the heat.
Heat Treatment
NO HEAT TREATMENT
Mechanical Properties
| Property | EN 10295Edition 2002[1] |
|---|---|
| Yield Strength | ≥ 220 MPa |
| Tensile Strength | ≥ 450 MPa |
| Elongation | ≥ 8 % |
Notes
EN 10295 · Edition 2002
[1] All properties in this column: Room temperature
Welding Conditions
N/A
Applications
At the heat-resistant casting-family level, typical applications include custom cast components for elevated-temperature industrial service; suitability must be checked against the applicable specification and service conditions.