GX40CrNiSi25-12 (EN 1.4837) Austenitic Stainless Steel Casting Material

Austenitic Stainless Steel

Download MDS PDF · Request a Quote

Introduction

GX40CrNiSi25-12 is a heat-resistant austenitic stainless steel casting grade covered by EN 10295. Typical family applications include furnace fixtures, support elements and burner-assembly components.

FieldValue
DesignationGX40CrNiSi25-12 (EN 1.4837)
Material TypeStainless Steel
Sub TypeAustenitic Stainless Steel
Product Formcasting

Manufacturing Process

Investment Casting
Shell Molding Casting
Sand Casting

Equivalent Materials

N/A

Similar Materials

N/A

Reference Standards

StandardStandard TitleEditionSpecificationIdentifier
EN 10295Heat resistant steel castings2002GX40CrNiSi25-12—

Physical Properties

PropertyValue / UnitNoteSource
Density7.8 kg/dm³EN 10295
Specific Heat500 J/(kg·K)Temperature: 20 °CEN 10295
Thermal Conductivity14 W/(m·K)Temperature: 20 °CEN 10295
Thermal Conductivity15 W/(m·K)Temperature: 100 °CEN 10295
Thermal Conductivity25.4 W/(m·K)Temperature: 800 °CEN 10295
Thermal Conductivity28.8 W/(m·K)Temperature: 1000 °CEN 10295
Thermal Expansion17.5 ×10⁻⁶/KTemperature range: 20–400 °CEN 10295
Thermal Expansion18.4 ×10⁻⁶/KTemperature range: 20–800 °CEN 10295
Thermal Expansion19.3 ×10⁻⁶/KTemperature range: 20–1000 °CEN 10295

Chemical Composition

ElementEN 10295Edition 2002 · wt.%Cast analysis
C0.30–0.50
Si1.00–2.50
Mn≤ 2.00
P≤ 0.040
S≤ 0.030
Cr24.00–27.00
Ni11.00–14.00
Mo≤ 0.50
Cu≤ 0.25[1]
Nb≤ 0.60[1]
V≤ 0.12[1]
W≤ 0.60[1]
Co≤ 1.00[1]

Notes

EN 10295 · Edition 2002

[1] Cu/Nb/V/W/Co: Unless otherwise agreed: limit for element unspecified in; no intentional addition except for finishing the heat.

Heat Treatment

EN 10295–2002

N/A

Mechanical Properties

Core Mechanical Properties

EN 10295 — 2002 · Table 2 — Normative

PropertyAs cast / no heat treatment
Yield Strength≥ 220 MPa
Tensile Strength≥ 450 MPa
Elongation≥ 6 %
Notes
  • Room temperature

Additional Mechanical Properties

Creep & Stress-Rupture Properties
PropertyValue / unitTemperature / conditionsNatureSource / editionNotes
σr — mean rupture stress100 MPaTemperature: 700 °C; Load time: 100 hInformativeEN 10295–2002 · EN 10295:2002, Annex B, Table B.1 (informative)Mean values; ±20% scatter band; information only, not acceptance requirements; Mean creep values from a scatter band of ±20%; information only.
σr — mean rupture stress80 MPaTemperature: 700 °C; Load time: 1000 hInformativeEN 10295–2002 · EN 10295:2002, Annex B, Table B.1 (informative)Mean values; ±20% scatter band; information only, not acceptance requirements; Mean creep values from a scatter band of ±20%; information only.
σ1% — mean stress for 1% elongation50 MPaTemperature: 700 °C; Load time: 10000 hInformativeEN 10295–2002 · EN 10295:2002, Annex B, Table B.1 (informative)Mean values; ±20% scatter band; information only, not acceptance requirements; Mean creep values from a scatter band of ±20%; information only.
σr — mean rupture stress70 MPaTemperature: 800 °C; Load time: 100 hInformativeEN 10295–2002 · EN 10295:2002, Annex B, Table B.1 (informative)Mean values; ±20% scatter band; information only, not acceptance requirements; Mean creep values from a scatter band of ±20%; information only.
σr — mean rupture stress40 MPaTemperature: 800 °C; Load time: 1000 hInformativeEN 10295–2002 · EN 10295:2002, Annex B, Table B.1 (informative)Mean values; ±20% scatter band; information only, not acceptance requirements; Mean creep values from a scatter band of ±20%; information only.
σ1% — mean stress for 1% elongation26 MPaTemperature: 800 °C; Load time: 10000 hInformativeEN 10295–2002 · EN 10295:2002, Annex B, Table B.1 (informative)Mean values; ±20% scatter band; information only, not acceptance requirements; Mean creep values from a scatter band of ±20%; information only.
σr — mean rupture stress45 MPaTemperature: 900 °C; Load time: 100 hInformativeEN 10295–2002 · EN 10295:2002, Annex B, Table B.1 (informative)Mean values; ±20% scatter band; information only, not acceptance requirements; Mean creep values from a scatter band of ±20%; information only.
σr — mean rupture stress25 MPaTemperature: 900 °C; Load time: 1000 hInformativeEN 10295–2002 · EN 10295:2002, Annex B, Table B.1 (informative)Mean values; ±20% scatter band; information only, not acceptance requirements; Mean creep values from a scatter band of ±20%; information only.
σ1% — mean stress for 1% elongation13 MPaTemperature: 900 °C; Load time: 10000 hInformativeEN 10295–2002 · EN 10295:2002, Annex B, Table B.1 (informative)Mean values; ±20% scatter band; information only, not acceptance requirements; Mean creep values from a scatter band of ±20%; information only.
σr — mean rupture stress26 MPaTemperature: 1000 °C; Load time: 100 hInformativeEN 10295–2002 · EN 10295:2002, Annex B, Table B.1 (informative)Mean values; ±20% scatter band; information only, not acceptance requirements; Mean creep values from a scatter band of ±20%; information only.
σr — mean rupture stress15 MPaTemperature: 1000 °C; Load time: 1000 hInformativeEN 10295–2002 · EN 10295:2002, Annex B, Table B.1 (informative)Mean values; ±20% scatter band; information only, not acceptance requirements; Mean creep values from a scatter band of ±20%; information only.
σ1% — mean stress for 1% elongation6 MPaTemperature: 1000 °C; Load time: 10000 hInformativeEN 10295–2002 · EN 10295:2002, Annex B, Table B.1 (informative)Mean values; ±20% scatter band; information only, not acceptance requirements; Mean creep values from a scatter band of ±20%; information only.

Welding Conditions

N/A

Applications

Austenitic stainless steel EN 10295 GX40CrNiSi25-12 is typically used for furnace hearth inserts and rails. EN 10295:2002 gives an informative maximum use temperature in air of 1050 °C, based on oxidation resistance in clean natural air. These figures are not guaranteed continuous or intermittent service temperatures, or allowable temperatures under load; other atmospheres require separate assessment.

Other cast components used in this material family include furnace fixtures, support elements and burner-assembly components. These applications include industrial heating and heat-treatment equipment. Atmosphere, loading, direct flame exposure, cyclic operation and process deposits must be considered separately from an in-air reference temperature.

Need GX40CrNiSi25-12 Castings?

Contact us for casting and machining inquiries.

Last Updated: November 6, 2026

error: Alert: Thanks for your interesting, but Article is protected ! You can click the Top Right email!