GX40CrNiSi22-10 (EN 1.4826) Austenitic Stainless Steel Casting Material

Austenitic Stainless Steel

Download MDS PDF · Request a Quote

Introduction

EN 10295 Grade GX40CrNiSi22-10 is a heat-resistant austenitic stainless steel casting grade. Process options include investment casting, shell molding and sand casting. Typical uses include heat-resistant cast components.

FieldValue
DesignationGX40CrNiSi22-10 (EN 1.4826)
Material TypeStainless Steel
Sub TypeAustenitic Stainless Steel
Product Formcasting

Manufacturing Process

Investment Casting
Shell Molding Casting
Sand Casting

Equivalent Materials

Not Available

Similar Materials

Not Available

Reference Standards

StandardStandard TitleEditionSpecificationIdentifier
EN 10295Heat resistant steel castings2002GX40CrNiSi22-10EN 1.4826

Physical Properties

PropertyValueApplicable Conditions
Density7.8 kg/dm³[1]
Thermal Conductivity14 W/(m·K)[1]Test temperature: 20 °C
Thermal Conductivity15 W/(m·K)[1]Test temperature: 100 °C
Thermal Conductivity25.4 W/(m·K)[1]Test temperature: 800 °C
Thermal Conductivity28.8 W/(m·K)[1]Test temperature: 1000 °C
Specific Heat500 J/(kg·K)[1]Test temperature: 20 °C
Thermal Expansion17.2 ×10⁻⁶/K[1]Temperature range: 20–400 °C
Thermal Expansion18.3 ×10⁻⁶/K[1]Temperature range: 20–800 °C
Thermal Expansion18.8 ×10⁻⁶/K[1]Temperature range: 20–1000 °C

Notes

  • [1] Informative values; not mandatory acceptance limits.

Chemical Composition

ElementRequirement
C0.30–0.50 %[1]
Si1.00–2.50 %[1]
Mn≤ 2.00 %[1]
P≤ 0.040 %[1]
S≤ 0.030 %[1]
Cr21.00–23.00 %[1]
Ni9.00–11.00 %[1]
Mo≤ 0.50 %[1]
Cu≤ 0.25 %[2]
V≤ 0.12 %[2]
Nb≤ 0.60 %[2]
W≤ 0.60 %[2]
Co≤ 1.00 %[2]

Notes

  • [1] C; Si; Mn; P; S; Cr; Mo; Ni: cast analysis
  • [2] W; Nb; V; Cu; Co: Unless otherwise agreed: limit for element unspecified in Table 1; no intentional addition except for finishing the heat.; cast analysis

Heat Treatment

EN 10295–2002

Not Available

Mechanical Properties

Primary Mechanical Properties

EN 10295 — 2002

Condition: Room temperature; As cast / no heat treatment

PropertyRequirement
Yield Strength≥ 230 MPa[1]
Tensile Strength≥ 450 MPa
Elongation≥ 8 %

Notes

  • [1] Yield Strength: Yield strength is 0.2% proof strength.

Additional Mechanical Properties

EN 10295 — 2002

Creep & Stress-Rupture Properties

Condition: 10000 h

Informative

Property600 °C700 °C800 °C900 °C
σ1% — mean stress for 1% elongation82 MPa[1][2][3][4]46 MPa[1][2][3][4]23 MPa[1][2][3][4]10 MPa[1][2][3][4]

Notes

  • [1] Mean creep values from a scatter band of ±20%; information only.
  • [2] Mean values
  • [3] ±20% scatter band
  • [4] information only, not acceptance requirements

Welding Conditions

Not Available

Applications

Austenitic stainless steel EN 10295 GX40CrNiSi22-10 is used for heat-resistant cast components. EN 10295:2002 gives an informative maximum use temperature in air of 950 °C, based on oxidation resistance in clean natural air. These figures are not guaranteed continuous or intermittent service temperatures, or allowable temperatures under load; other atmospheres require separate assessment.

Other cast components used in this material family include furnace fixtures, support elements and burner-assembly components. These applications include industrial heating and heat-treatment equipment. Atmosphere, loading, direct flame exposure, cyclic operation and process deposits must be considered separately from an in-air reference temperature.

Need GX40CrNiSi22-10 Castings?

Contact us for casting and machining inquiries.

Last Updated: November 25, 2026

error: Alert: Thanks for your interesting, but Article is protected ! You can click the Top Right email!