GX30CrSi7 (EN 1.4710) Alloy Steel Casting Material

Alloy Steel

Download MDS PDF · Request a Quote

Introduction

GX30CrSi7 is a heat-resistant alloy steel casting grade covered by EN 10295. Typical family applications include furnace fixtures, support elements and burner-assembly components.

FieldValue
DesignationGX30CrSi7 (EN 1.4710)
Material TypeAlloy Steel
Sub Type—
Product Formcasting

Manufacturing Process

Investment Casting
Shell Molding Casting
Sand Casting

Equivalent Materials

N/A

Similar Materials

N/A

Reference Standards

StandardStandard TitleEditionSpecificationIdentifier
EN 10295Heat resistant steel castings2002GX30CrSi7—

Physical Properties

PropertyValue / UnitNoteSource
Density7.7 kg/dm³EN 10295
Specific Heat460 J/(kg·K)Temperature: 20 °CEN 10295
Thermal Conductivity24 W/(m·K)Temperature: 20 °CEN 10295
Thermal Expansion12.5 ×10⁻⁶/KTemperature range: 20–400 °CEN 10295
Thermal Expansion13.5 ×10⁻⁶/KTemperature range: 20–800 °CEN 10295

Chemical Composition

ElementEN 10295Edition 2002 · wt.%Cast analysis
C0.20–0.35
Si1.00–2.50
Mn0.50–1.00
P≤ 0.035
S≤ 0.030
Cr6.00–8.00
Ni≤ 0.50
Mo≤ 0.15
Cu≤ 0.20[1]
Nb≤ 0.20[1]
V≤ 0.08[1]
W≤ 0.20[1]
Co≤ 0.50[1]

Notes

EN 10295 · Edition 2002

[1] Cu/Nb/V/W/Co: Unless otherwise agreed: limit for element unspecified in; no intentional addition except for finishing the heat.

Heat Treatment

EN 10295–2002 · +A

StepOperationTemperatureCooling
1anneal800–850 °C—

Mechanical Properties

Core Mechanical Properties

N/A

Additional Mechanical Properties

Creep & Stress-Rupture Properties
PropertyValue / unitTemperature / conditionsNatureSource / editionNotes
σ1% — mean stress for 1% elongation19 MPaTemperature: 600 °C; Load time: 10000 hInformativeEN 10295–2002 · EN 10295:2002, Annex B, Table B.1 (informative)Mean values; ±20% scatter band; information only, not acceptance requirements; Mean creep values from a scatter band of ±20%; information only.
σ1% — mean stress for 1% elongation8 MPaTemperature: 700 °C; Load time: 10000 hInformativeEN 10295–2002 · EN 10295:2002, Annex B, Table B.1 (informative)Mean values; ±20% scatter band; information only, not acceptance requirements; Mean creep values from a scatter band of ±20%; information only.
σ1% — mean stress for 1% elongation2.5 MPaTemperature: 800 °C; Load time: 10000 hInformativeEN 10295–2002 · EN 10295:2002, Annex B, Table B.1 (informative)Mean values; ±20% scatter band; information only, not acceptance requirements; Mean creep values from a scatter band of ±20%; information only.

EN 10295–2002 · +A

N/A

Welding Conditions

EN 10295–2002

RequirementValue
Preheat300–500 °C[1]
Post-weld Heat TreatmentStress relief annealing at 760 °C to 800 °C[2]

EN 10295:2002, Annex A, Table A.1 (informative)

Notes

EN 10295 · Edition 2002

[1] Preheat: Production welding; informative; The welded area should not cool below the minimum preheat temperature before post-weld heat treatment.

[2] Post-weld Heat Treatment: Production welding; informative

Applications

Alloy steel EN 10295 GX30CrSi7 is typically used for burner and stove components. EN 10295:2002 gives an informative maximum use temperature in air of 750 °C, based on oxidation resistance in clean natural air. These figures are not guaranteed continuous or intermittent service temperatures, or allowable temperatures under load; other atmospheres require separate assessment.

Other cast components used in this material family include furnace fixtures, support elements and burner-assembly components. These applications include industrial heating and heat-treatment equipment. Atmosphere, loading, direct flame exposure, cyclic operation and process deposits must be considered separately from an in-air reference temperature.

Need GX30CrSi7 Castings?

Contact us for casting and machining inquiries.

Last Updated: November 6, 2026

error: Alert: Thanks for your interesting, but Article is protected ! You can click the Top Right email!