CC50 Ferritic Stainless Steel Casting Material

Ferritic Stainless Steel

Download MDS PDF · Request a Quote

Introduction

ASTM A743 Grade CC50 is a ferritic stainless steel grade. Process options include investment casting, shell molding and sand casting. Typical uses include pump casings, impellers, valve bodies and seats in chemical manufacturing, mining and pulp-and-paper equipment.

FieldValue
DesignationCC50
Material TypeStainless Steel
Sub TypeFerritic Stainless Steel
Product Formcasting

Manufacturing Process

Investment Casting
Shell Molding Casting
Sand Casting

Equivalent Materials

Not Available

Similar Materials

Not Available

Reference Standards

StandardStandard TitleEditionSpecificationIdentifier
ASTM A743Standard Specification for Castings, Iron-Chromium, Iron-Chromium-Nickel, Corrosion Resistant, for General Application03CC50UNS J92615

Physical Properties

Not Available

Chemical Composition

ElementRequirement
C≤ 0.50 %
Si≤ 1.50 %
Mn≤ 1.00 %
P≤ 0.04 %
S≤ 0.04 %
Cr26.0–30.0 %
Ni≤ 4.00 %

Heat Treatment

Heat TreatmentOperationTemperatureCooling
Air cooling alternativeHeat[1]≥ 1450°F [790°C]air

Notes

  • [1] Heat: and air cool; or (2) Heat to 1450°F [790°C] minimum; and furnace cool.
Heat TreatmentOperationTemperatureCooling
Furnace cooling alternativeHeat[1]≥ 1450°F [790°C]furnace

Notes

  • [1] Heat: and air cool; or (2) Heat to 1450°F [790°C] minimum; and furnace cool.

Mechanical Properties

Primary Mechanical Properties

ASTM A743 — 03

Condition: heat treatment per Table 1

PropertyRequirement
Tensile Strength≥ 55 ksi [380 MPa][1][2]

Notes

  • [1] separately cast keel block per S12.2 unless S12.3 agreement applies
  • [2] Applies only when Supplementary Requirement S12 is specified

ASTM A743 — 03

Condition: non-austenitic grade; Table 1 treatment

PropertyRequirement
Brinell Hardness≤ 241 HB[1][2]

Notes

  • [1] per manufacturer–purchaser agreement (S14.2)
  • [2] Applies only when Supplementary Requirement S14 is specified

Welding Conditions

Not Available

Applications

Ferritic stainless steel ASTM A743 Grade CC50 is used for pump casings, impellers, valve bodies and seats in chemical manufacturing, mining and pulp-and-paper equipment. Other documented castings include bushings, cylinder liners and digester parts. Other cast components used in this material family include stationary pump casings, valve components and sleeves.

Typical industrial settings include chemical processing, mining and pulp-and-paper equipment. Aggressive liquids, sliding contact and suspended solids require assessment for the particular service.

Need CC50 Castings?

Contact us for casting and machining inquiries.

Last Updated: November 25, 2026

error: Alert: Thanks for your interesting, but Article is protected ! You can click the Top Right email!