70-40 [485-275] Carbon Steel Casting Material

Carbon Steel

Download MDS PDF · Request a Quote

Introduction

ASTM A27/A27M Grade 70-40 [485-275] is a heat-treated carbon steel for castings. The standard specifies a minimum yield point as well as tensile strength, elongation and reduction of area.

FieldValue
Designation70-40 [485-275]
Material TypeCarbon Steel
Sub TypeSteel
Product Formcasting

Manufacturing Process

Investment Casting
Shell Molding Casting
Sand Casting

Equivalent Materials

Not Available

Similar Materials

Not Available

Reference Standards

StandardStandard TitleEditionSpecificationIdentifier
ASTM A27/A27MSteel Castings, Carbon, for General Application1370-40 [485-275]UNS J02501

Physical Properties

Not Available

Chemical Composition

ElementRequirement
C≤ 0.25 %
Si≤ 0.80 %
Mn≤ 1.20 %[1]
P≤ 0.035 %
S≤ 0.035 %

Notes

  • [1] Mn: For every 0.01 % below the maximum carbon, 0.04 % above the manganese limit is permitted, up to 1.40 % Mn.
ElementASTM A27/A27M — 13 — Conditional requirements
Cr≤ 0.50 %[2]
Ni≤ 0.50 %[2]
Mo≤ 0.25 %[2]
Cu≤ 0.50 %[1]

Notes

  • [1] Cu: Applies only when Supplementary Requirement S54 is specified; When S54 applies, combined Cu + Ni + Mo + Cr shall not exceed 1.00 %.
  • [2] Ni; Mo; Cr: Applies only when Supplementary Requirement S54 is specified

Heat Treatment

Required heat treatment — Full annealing, normalizing, normalizing and tempering, or quenching and tempering. Unless otherwise specified, one or a combination may be selected by the manufacturer. Cool below the transformation range from pouring temperature before heat treatment. Furnace temperature is regulated using pyrometers. If castings are retreated after a failed mechanical test, no more than three reaustenitizations are allowed without purchaser approval.

Mechanical Properties

Primary Mechanical Properties

ASTM A27/A27M — 13

PropertyInch-pound 70-40 (ksi)SI 485-275 (MPa)
Tensile Strength≥ 70 ksi[1]≥ 485 MPa[1]
Yield Strength≥ 40 ksi[1]≥ 275 MPa[1]
Elongation≥ 22 %[1][2]≥ 22 %[1][3]
Reduction of Area≥ 30 %[1]≥ 30 %[1]

Notes

  • [1] Same heat as the represented casting
  • [2] Elongation [Inch-pound 70-40 (ksi)]: Minimum elongation measured over 2 in. For ICI test bars the gauge length to reduced section diameter ratio is 4:1.
  • [3] Elongation [SI 485-275 (MPa)]: Minimum elongation measured over 50 mm. For ICI test bars the gauge length to reduced section diameter ratio is 4:1.

Welding Conditions

ASTM A27/A27M — 13

PropertyRequirement
Post-weld Heat TreatmentClass 1 when postweld heat treatment is required; identify the welds to be treated. Class 2 when it is not required.

Applications

Carbon steel ASTM A27/A27M Grade 70-40 [485-275] is one of the carbon steel casting grades for general application. The broader material family is used in pump and valve parts and in construction equipment. The cited uses have no grade-specific service rating.

Need 70-40 [485-275] Castings?

Contact us for casting and machining inquiries.

Last Updated: November 25, 2026

error: Alert: Thanks for your interesting, but Article is protected ! You can click the Top Right email!