Introduction
ASTM A27/A27M Grade 70-36 [485-250] is a carbon steel casting grade. Its designation identifies the tensile and yield levels, and the grade also carries ductility requirements.
| Field | Value |
|---|---|
| Designation | 70-36 [485-250] |
| Material Type | Carbon Steel |
| Sub Type | Steel |
| Product Form | casting |
Manufacturing Process
Investment Casting
Shell Molding Casting
Sand Casting
Equivalent Materials
Not Available
Similar Materials
Not Available
Reference Standards
| Standard | Standard Title | Edition | Specification | Identifier |
|---|---|---|---|---|
| ASTM A27/A27M | Steel Castings, Carbon, for General Application | 13 | 70-36 [485-250] | UNS J03501 |
Related Casting Products
Physical Properties
Not Available
Chemical Composition
| Element | Requirement |
|---|---|
| C | ≤ 0.35 % |
| Si | ≤ 0.80 % |
| Mn | ≤ 0.70 %[1] |
| P | ≤ 0.035 % |
| S | ≤ 0.035 % |
Notes
- [1] Mn: For every 0.01 % below the maximum carbon, 0.04 % above the manganese limit is permitted, up to 1.00 % Mn.
| Element | ASTM A27/A27M — 13 — Conditional requirements |
|---|---|
| Cr | ≤ 0.50 %[2] |
| Ni | ≤ 0.50 %[2] |
| Mo | ≤ 0.25 %[2] |
| Cu | ≤ 0.50 %[1] |
Notes
- [1] Cu: Applies only when Supplementary Requirement S54 is specified; When S54 applies, combined Cu + Ni + Mo + Cr shall not exceed 1.00 %.
- [2] Ni; Mo; Cr: Applies only when Supplementary Requirement S54 is specified
Heat Treatment
Required heat treatment — Full annealing, normalizing, normalizing and tempering, or quenching and tempering. Unless otherwise specified, one or a combination may be selected by the manufacturer. Cool below the transformation range from pouring temperature before heat treatment. Furnace temperature is regulated using pyrometers. If castings are retreated after a failed mechanical test, no more than three reaustenitizations are allowed without purchaser approval.
Mechanical Properties
Primary Mechanical Properties
ASTM A27/A27M — 13
| Property | Inch-pound 70-36 (ksi) | SI 485-250 (MPa) |
|---|---|---|
| Tensile Strength | ≥ 70 ksi[1] | ≥ 485 MPa[1] |
| Yield Strength | ≥ 36 ksi[1] | ≥ 250 MPa[1] |
| Elongation | ≥ 22 %[1][2] | ≥ 22 %[1][3] |
| Reduction of Area | ≥ 30 %[1] | ≥ 30 %[1] |
Notes
- [1] Same heat as the represented casting
- [2] Elongation [Inch-pound 70-36 (ksi)]: Minimum elongation measured over 2 in. For ICI test bars the gauge length to reduced section diameter ratio is 4:1.
- [3] Elongation [SI 485-250 (MPa)]: Minimum elongation measured over 50 mm. For ICI test bars the gauge length to reduced section diameter ratio is 4:1.
Welding Conditions
ASTM A27/A27M — 13
| Property | Requirement |
|---|---|
| Post-weld Heat Treatment | Class 1 when postweld heat treatment is required; identify the welds to be treated. Class 2 when it is not required. |
Applications
Carbon steel ASTM A27/A27M Grade 70-36 [485-250] belongs to a family of steel castings used in mining machinery and power-generation equipment. These examples describe industrial uses of cast carbon steels without specifying a grade for an individual component.
Need 70-36 [485-250] Castings?
Contact us for casting and machining inquiries.
Email Us for a QuoteLast Updated: November 25, 2026