Introduction
60-42-10 is a ductile cast iron grade covered by ASTM A536. Typical family applications include pipe fittings, connection pieces, valve bodies and coupling housings.
| Field | Value |
|---|---|
| Designation | 60-42-10 |
| Material Type | Cast Iron |
| Sub Type | Ductile Cast Iron |
| Product Form | casting |
Manufacturing Process
Sand Casting
Shell Molding Casting
Lost Foam Casting
Equivalent Materials
N/A
Similar Materials
N/A
Reference Standards
| Standard | Standard Title | Edition | Specification | Identifier |
|---|---|---|---|---|
| ASTM A536 | Standard Specification for Ductile Iron Castings | 84(1999)e1 | 60-42-10 | — |
Related Casting Products
Physical Properties
N/A
Chemical Composition
No specified chemical composition limits in ASTM A536
Heat Treatment
ASTM A536–84(1999)e1
N/A
Mechanical Properties
Core Mechanical Properties
ASTM A536 — 84(1999)e1 · Table 2 — Normative
- Standard round tensile specimen, 2 in. or 50 mm gauge length; small-size alternatives for 1/2-in. Y-block per Clause 11.1; Special applications, such as pipes and fittings; Test coupons represent the same ladle or heat and receive the same thermal treatment as the castings. Coupon size is selected by the purchaser, or by the manufacturer if not specified. No quantitative coupon-to-casting property relationship is prescribed.
ASTM A536 — 84(1999)e1 · Table 2 — Informative
- Standard round tensile specimen, 2 in. or 50 mm gauge length; small-size alternatives for 1/2-in. Y-block per Clause 11.1; Special applications, such as pipes and fittings; Test coupons represent the same ladle or heat and receive the same thermal treatment as the castings. Coupon size is selected by the purchaser, or by the manufacturer if not specified. No quantitative coupon-to-casting property relationship is prescribed.
Notes
ASTM A536 · Edition 84(1999)e1
[1] Tensile Strength: Chemical requirements may be agreed between manufacturer and purchaser. Hardness requirements apply only when specified in the contract or purchase order; no numerical hardness limit is prescribed. Special microstructure, pressure-tightness, radiographic, magnetic-particle, dimensional and surface-finish requirements apply only when specified in the contract or purchase order.
[2] Yield Strength: Yield strength is determined at 0.2% offset; another method requires mutual agreement.
[3] Elongation: Elongation gauge length: 2 in. or 50 mm. For a 1/2-in. Y-block use a permitted small-size specimen.
[4] Tensile Strength: The inch-pound values govern. SI values reproduce the printed and are not independent requirements.; Informative reference value; not an acceptance requirement
[5] Yield Strength: Yield strength is determined at 0.2% offset; another method requires mutual agreement.; The inch-pound values govern. SI values reproduce the printed and are not independent requirements.; Informative reference value; not an acceptance requirement
Welding Conditions
N/A
Applications
Ductile cast iron ASTM A536 Grade 60-42-10: ASTM A536 lists this grade for special applications such as pipes and fittings. Commercial documentation also identifies grade 60-42-10 in water-service wall-pipe assemblies; the separate product specification determines the detailed pipe requirements. Other cast components used in this material family include pipe fittings, connection pieces, valve bodies and coupling housings.
Applications include water-distribution pipelines, wastewater systems and industrial fluid-handling assemblies. Product-specific pressure classes, coatings, linings and joint details remain applicable.