SS321 is not a Casting Grade in ASTM A351 and A743 standard, just listed in ASTM A182 and ASTM A240. SS321 contains titanium for chromium carbide stabilization. Generally Ti will oxidize rapidly in the melt if exposed to air in typical sand/investment casting processes, but based on the little content, it’s no problem in our Casting process.
We will follow the SS321 Casting material as below standard.
www.castingquality.com
Casting Quality Industrial provide Sand Casting and Precision Investment Casting for this special stainless steel.
Our Services
- Sand Casting
Casting Quality focus on Metal Parts industry, we provide professional service in Metal Casting field.
Sand Casting is a popular metal form method, are suitable for all materiel, such as grey iron, ductile iron, malleable iron, carbon steel, stainless steel, aluminum and bronze.
- Investment Casting
also named as precision lost wax casting, mainly suitalbe for carbon steel and stainless steel parts. We also provide grey iron and ductile iron and aluminum and bronze parts by investment casting. It can achieve the best appearance with good tolerance
- Shell Casting
Shell casting method is a good option to replace investment casting and sand casting. the quality is better than sand casting parts, suitable for bulk production.
- CNC Machining
CNC Milling, CNC turning with 5 xix CNC center, we provide precision machining for all castings based on customers design drawings.
- CAD Design
Mechanical Design service based on customers requirement, our software is Solidworks and AutoCAD.
- Tools/Mold Design
Mould design and production will be served for metal casting ad plastic injection industry. Based on our more than 10 years experience, we supply professional molds for our customers in Europe and North American.
Stainless Steel SS321 Description
Similar Metal grade in different application:
UNS | Grade | BS | EN | DIN | DIN | JIS | China |
S32100 | 321 | 321S31 | 58B | 1.4541 | X6CrNiTi8-10 | SUS321 | 0Cr18Ni9Ti |
S32109 | 321H | 321S51 | – | 1.4878 | X10CrNiTi8-10 | SUS321H | 1Cr18Ni9Ti |
www.castingquality.com
ASTM A240 – Standard Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications
ASTM A182 -Standard Specification for Forged or Rolled Alloy-Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service
SS321 Chemical Composition Requirements, %
Standard | Grade | UNS | C | Mn | P | S | Si | Ni | Cr | N | Ti |
ASTM 182 | F321 | S32100 | 0.08 | 2.00 | 0.045 | 0.030 | 1.00 | 9.0-12.0 | 17.0-19.0 | 0.70 | |
F321H | S32109 | 0.04-0.10 | 2.00 | 0.045 | 0.030 | 1.00 | 9.0-12.0 | 17.0-19.0 | 0.70 | ||
ASTM A240 | 321 | S32100 | 0.08 | 2.00 | 0.045 | 0.030 | 0.75 | 9.0-12.0 | 17.0-19.0 | 0.1 | 0.70 |
321H | S32109 | 0.04-0.10 | 2.00 | 0.045 | 0.030 | 0.75 | 9.0-12.0 | 17.0-19.0 | 0.70 |
Grade F 321 shall have a titanium content of not less than five times the carbon content and not more than 0.70 %.
Grade F 321H shall have a titanium content of not less than 4 times the carbon content and not more than 0.70 %.
Grade SS321: Ti 5 x(C+N), MIN, 0.70 max) www.castingquality.com
Grade SS321H: Ti 4 x (C+N) min, 0.70 max) www.castingquality.com
SS321 Mechanical Test Requirements
Standard | Grade | UNS | Tensile Ksi | Tensile Mpa | Yield Ksi | Yield MPa | Elongation | Reduction | Hardness Brinel | Hardness Rockwell B |
ASTM 182 | F321 | S32100 | 75 | 515 | 30 | 205 | 30 | 50 | – | – |
F321H | S32109 | 75 | 515 | 30 | 205 | 30 | 50 | – | – | |
ASTM A240 | 321 | S32100 | 75 | 515 | 30 | 205 | 40.0 | – | 217 | 95 |
321H | S32109 | 75 | 515 | 30 | 205 | 40.0 | – | – | – |
www.castingquality.com
SS321 Heat treatment process: Solution treat and Quench, Heat to 1900°F [1040°C] minimum, hold for sufficient time to heat casting to temperature, quench in water or rapid cool by other means (Quenching cool below 500°F [260°C]) www.castingquality.com
Manufacture process in Qingdao Casting Quality company: Sand Casting, Precision Investment Casting (Lost Wax Casting).
www.castingquality.com
Why Choose Stainless Steel 321?Sometime, SS321 is basic austenitic stainless steel 304 with Titanium content, but SS321 has better property in application in temperature up to 900°C. Titanium gives it greater inter-granular corrosion resistance; this grades perform well in the 425-900 °C range. 304L is not good for high temperature strength, mainly for resistance to intergranular corrosion.